晋艳娟, 崔小朝, 李朗, et al. Coupled Numerical Simulation of Flow Field and Temperature Field in Slab Concasting Filling Process[J]. Special Steel, 2006, 27(5): 6-8.
晋艳娟, 崔小朝, 李朗, et al. Coupled Numerical Simulation of Flow Field and Temperature Field in Slab Concasting Filling Process[J]. Special Steel, 2006, 27(5): 6-8.DOI:
The flow and solidification status of molten steel with coupling flow field and temperature field in inner- outer couple cooling mold has been simulated by using CFD commercial code Flow-3 d software to get distributing diagrams of flow field and temperature
and free-surface level and shape diagram. The influence of flow field and temperature field in slab concasting filling process on solidification of molten steel was analyzed. It is indicated that the inner cooler could improve the molten steel flow status which is favourable for inclusion floating up in molten steel and increasing the solidification rate of molten steel