龚殿尧, 徐建忠, 郑晖, et al. A Short-cut Calculation Method for Finishing Rolling Temperature Control of Hot Rolled Strip[J]. Special Steel, 2007, 28(2): 31-33.
龚殿尧, 徐建忠, 郑晖, et al. A Short-cut Calculation Method for Finishing Rolling Temperature Control of Hot Rolled Strip[J]. Special Steel, 2007, 28(2): 31-33.DOI:
The temperature of hot strip at finishing rolling interstand has been calculated by established short-cut calculation model and defined concept of equivalent interstand distance and fundamental value. The comparison between shortcut method calculated results and theory model calculated results showed that the temperature of hot strip at finishing rolling region could be calculated accurately. As target temperature is changed the status of cooling jet at interstand can be adjusted by short-cut calculation method to fit in with new target temperature.