齐殿威, 牟昊, 丁伟. Recent Progress of Research and Development on Production Process for Grain-Oriented Electrical Steel Sheets in Japan[J]. Special Steel, 2011, 32(2): 21-26.
齐殿威, 牟昊, 丁伟. Recent Progress of Research and Development on Production Process for Grain-Oriented Electrical Steel Sheets in Japan[J]. Special Steel, 2011, 32(2): 21-26.DOI:
According to related typical patent technology for grain-oriented electrical steel sheets
the recent trends and progress situation for production process of grain-oriented electrical steel sheets with high magnetic flux density and low core loss in Japan are summarized including low temperature slab heating
suitably regulating inhibitors
.adjusting and utilizing key element Mn
C
Sn and Sb
manufacturing for new annealing agent and insulating solutions
and fining magnetic domain
and some suggestions are put for domestic grain-oriented electric steel producer to apply for a patent.