光红兵, 张文康, 辛宪诚, et al. Effect of Rare Earth Element on Structure and Magnetic Performance of Cold Rolled Non-Oriented Electrical Steel Products[J]. Special Steel, 2012, 33(2): 58-61.
光红兵, 张文康, 辛宪诚, et al. Effect of Rare Earth Element on Structure and Magnetic Performance of Cold Rolled Non-Oriented Electrical Steel Products[J]. Special Steel, 2012, 33(2): 58-61.DOI:
Rare earth element ( RE) wire is fed to electric steel liquid (/% : ≤ 0.005C
2.0-2.6Si
0.20-0.30Mn
0.008P
0.001-0.009S
0.15-0.40Al
≤0.0010[O] ) in mold by auto feeding wire machine through a side tube at 220 mm x 1 280 mm curved caster. Effect of rare earth element content (0-0.45% RE) on structure and texture
morphology and distribution of inclusions
and magnetic performance of 0.5 mm annealed cold rolled non-oriented electrical steel products is systematically studied by optical and electric microscope. Results show that 0.008%-0.020% rare elements in steel
it is available to effectively control the harmful effect of fine inclusions in steel
promote increasing of grain size of annealed products
to intensify favorable texture ingredient and obviously improve magnetic performance of cold rolled non-oriented electrical steel products.