苑阳阳, 黄进科, 张宇, 等. 合金工具钢S2盘条的开发[J]. 特殊钢, 2018,39(2):25-29.
苑阳阳, 黄进科, 张宇, et al. Development of Coil of Alloy Tool Steel S2[J]. Special Steel, 2018, 39(2): 25-29.
通过80 kg真空感应炉试验及Gleeble 3800热模拟试验机测试了连续冷却相转变(CCT)曲线
设计了S2钢的化学成分(/%:0.630.69C
1.001.20Si
0.400.60Mn
0.200.40Cr
0.400.50Mo
0.150.25V
0.100.30Ni
0.0100.030Nb
≤0.015P
≤0.010S)
并进行120t BOF-LF-VD-300 mm×390 mm方坯连铸-开坯-高线轧制-斯太尔摩控冷流程的工业性生产。通过铁水脱硫
铁水硫含量≤0.010%
BOF终点[C
]
0.10%0.30%
[P
]
≤0.012%
钢水终点温度1620~1660℃
BOF出钢采用Si-Mn预脱氧
LF精炼渣(/%:8~10MgO
44~45CaO
5~10SiO
2
25~35Al
2
O
3
LF精炼结束喂钙线
连铸钢水过热度≤25℃
拉速0.65m/min和轧制控冷等工艺措施
成功开发了合金工具钢S2盘条。检验结果表明
Φ8mm热轧盘条奥氏体晶粒度为8.5~9.0级
脱碳层厚度≤0.5%D
热轧盘条HRC硬度值50
同卷HRC硬度值波动小于6
各项性能满足技术要求。
By testing with a 80kg vacuum induction furnace and measuring continuous cooling transformation (CCT) curves by using Gleeble 3800 hot simulation machine the chemical composition of steel S2 (/%: 0.63~0.69C
1.00~1.20Si
0.40~0.60Mn
0.20~0.40Cr
0.40~0.50Mo
0.15~0.25V
0.10~0.30Ni
0.010~0.030Nb
≤0.015P
≤0.010S) has been designed
and the commercial production by 120t BOF-LF-VD-300mmx390mm bloom casting-breakdown-high speed wire rolling-Stelmor control cooling process has been carried out. With the process measures including hot metal dephosphorization
sulphur content in metal ≤0.010%
control of BOF end[C
]
0.10% ~0.30%
end[P
]
≤0.012%
liquid end temperature 1620~1660℃
using Si-Mn pre-deoxid
ation in BOF tapping
LF refining slag (/%: 8~10MgO
44~45CaO
5~10SiO
2
25~35Al
2
O
3
feeding calcium wire at end of LF refining
overheating extent of casting liquid ≤25℃,casting speed 0.65m/min
and controlling cooling after rolling
the cqil of alloy tool steel S2 is successfully developed. Examination results show that the each property index of Φ8mm hot-rolled coil meets the requirement of technical specification
including the austenite grain size rating 8.5~9.0
the depth of decarburization layer≤0.5%D
the HRC hardness value of hot-rolled coil 50 and the variation of HRC hardness value of same coil less than 6.