杨相歧, 庄迎, 李吉东, et al. Research on Grain Size Control of 316 Austenitic Stainless Steel Heavy and Medium Plate Rolling[J]. Special Steel, 2019, 40(3): 70-73.
杨相歧, 庄迎, 李吉东, et al. Research on Grain Size Control of 316 Austenitic Stainless Steel Heavy and Medium Plate Rolling[J]. Special Steel, 2019, 40(3): 70-73.DOI:
deformation rate per pass on grain of 316 austenitic stainless steel medium plate was done in laboratory. The results explained that the total compression ratio is more than 6
the original structure of steel billet has no influence on grain size of hot rolling plate
when the total compression ratio is more than 6
the homogeneous grain in the whole thickness is obtained in condition of same billet steel heating- up temperature and deformation rate per pass. But when the total compression ratio is more than 6
the 2 grade and 7 grade duplex grain are obtained even though the deformation rate per pass is more than 30%
and when the total compression ratio is less than 10%
the grain is heterogeneous even though the total compression ratio is big enough.