徐钦华, 彭科, 朱建新, et al. Effect of Pass Reduction Ratio Configurations on Martensitic Transformation During 304H Stainless Steel Wire Drawing[J]. Special Steel, 2020, 41(2): 57-61.
徐钦华, 彭科, 朱建新, et al. Effect of Pass Reduction Ratio Configurations on Martensitic Transformation During 304H Stainless Steel Wire Drawing[J]. Special Steel, 2020, 41(2): 57-61.DOI:
two different drawing processes (reduction of area /% :process No1
34. 45
31. 67
19
00 and 20.08;process No2
20. 10
19. 28
34. 64
31.41) are designed. The effects of pass reduction of area on martensitic transformation
magnetic properties and mechanical properties of 304H stainless steel in wire drawing are studied. The results show that when the total strain of the steel wire is the same
the large reduction ratio at first and second pass is more favorable for martensite transformation
and the saturation magnetization Ms is larger. Otherwise
the martensite transformation is less
and the saturation magnetization is smaller. The strength o£ the steel wire is linearly related to the true strain of the drawing
and the value is related only to the total strain of the drawing. In the test
as the first two pass reduction ratios are 20.10% and 19.28%
and the latter two pass reduction ratios are 34.64% and 31.41%
the martensite transformation is less and the saturation magnetization of the steel wire is weak.