陈均, 梁新腾. Test and Research on Improving Scrap Consumption of Converter During Semi Steel Steelmaking of 200 t BOF[J]. Special Steel, 2021, 42(6): 32-36.
陈均, 梁新腾. Test and Research on Improving Scrap Consumption of Converter During Semi Steel Steelmaking of 200 t BOF[J]. Special Steel, 2021, 42(6): 32-36.DOI:
According to low consumption of scrap consumption in semi-steel smelting converter at Panzhihua Steel caused by insufficient heat source of semi-steel
by calculating the heat balance of the converter
the theoretical scrap consumption under different semi-steel conditions and the corresponding relationship between the end-point carbon
temperature and scrap consumption are obtained.By charging silicon in semi-steel and using carbon during blowing for thermal compensation and adopting technical measures of optimized slag charging system
reducing tapping temperature
the carbon content at the end-point of molten steel has increased from 0.048% to0.068%
BOF tapping temperature reduced from 1658 ℃ to 1638℃
in the case of a lower material consumption of per ton steel
the dephosphorization rate increased by 1.1 percent- age point on average
and the scrap consumption increases from original 38.9 kg/t