1.钢铁研究总院有限公司特殊钢研究院,北京 100081
2.北京科技大学钢铁共性技术协同创新中心,北京 100083
迟宏宵(1983―),男,博士,正高级工程师;E-mail:chihongxiao@163.com
收稿:2023-05-31,
纸质出版:2023-10-01
移动端阅览
迟宏宵,刘继浩,马党参等.喷射成形技术在高合金工具钢中的应用及研究进展[J].特殊钢,2023,44(05):14-21.
Chi Hongxiao,Liu Jihao,Ma Dangshen,et al.Application and Research Progress of Spray Forming Technology in High Alloy Tool Steel[J].Special Steel,2023,44(05):14-21.
迟宏宵,刘继浩,马党参等.喷射成形技术在高合金工具钢中的应用及研究进展[J].特殊钢,2023,44(05):14-21. DOI: 10.20057/j.1003-8620.2023-00108.
Chi Hongxiao,Liu Jihao,Ma Dangshen,et al.Application and Research Progress of Spray Forming Technology in High Alloy Tool Steel[J].Special Steel,2023,44(05):14-21. DOI: 10.20057/j.1003-8620.2023-00108.
喷射成形是制备高性能高合金化工具钢的一种先进工艺技术,具备短流程、成本低、绿色化的技术优势。目前,喷射成形制备高合金工具钢在国内已逐步实现规模产业化。本文重点介绍了国内外喷射成形高合金工具钢的发展及研究进展;总结了喷射成形高速钢、模具钢的微观组织和力学性能特征;提出未来喷射成形高合金工具钢的发展应注重利用数字化、智能化等控制技术进一步提高产品的质量和性能稳定性,系统研究及建立合金成分-工艺参数-组织性能特征-服役应用的关系,并通过探索新工艺和新方法,发挥喷射成形的工艺优势及应用前景。
Spray forming is an advanced process technology for preparing high-performance and high alloy tool steel, which has the advantages of short process, low cost, and green technology. At present, the application of spray forming in high alloy tool steel in China has gradually achieved large-scale industrialization. This article focuses on the development and research progress of spray formed high alloy tool steel both domestically and internationally; Summarized the microstructure and mechanical properties of spray formed high-speed steel and mold steel; and proposed that the future development of spray forming technology in high alloy tool steel should focus on using digital and intelligent manufacturing technologies to further improve product quality and performance stability. To systematically study and establish the relationship between alloy composition, process parameters, microstructure and property characteristics and service application, and exploring new processes and methods to leverage the technological advantages and application prospects of spray forming.
Singer A R . Recent development in the spray forming of metals: Prat I [J]. MPR , 1986 , 2 : 109 - 122 .
Singer A R . Recent development in the spray forming of metals: Prat I [J]. MPR , 1986 , 3 : 223 - 336 .
Boccalini M , Goldenstein H . Solidification of high speed steels [J]. International Materials Reviews , 2001 , 46 ( 2 ): 92 - 115 .
朱喜达 , 陆家生 , 赵勇智 , 等 . 冷作模具钢(Cr12MoV)短流程生产工艺实践 [J]. 特殊钢 , 2023 , 44 ( 3 ): 10 - 13 .
Wang Y J , Chu S J , Mao B , et al . Microstructure, residual stress, and mechanical property evolution of a spray-formed vanadium-modified high-speed steel processed by post-heat treatment [J]. Journal of Materials Research and Technology , 2022 , 18 : 1521 - 1533 .
谢志彬 , 邵青立 , 张国平 , 等 . 快速抽锭电渣重熔M2高速钢160 mm×160 mm铸坯工艺及质量 [J]. 特殊钢 , 2019 , 40 ( 1 ): 47 - 51 .
刘友荣 . 降低工模具钢电渣重熔钢锭顶部缩孔缺陷的工艺实践 [J]. 特殊钢 , 2015 , 36 ( 4 ): 34 - 37 .
赵志刚 , 颜慧成 , 仇圣桃 , 等 . 冷却速率对M2高速工具钢铸锭凝固组织的影响 [J]. 特殊钢 , 2014 , 35 ( 3 ): 45 - 48 .
陈佳艺 , 朱雷敏 , 殷子豪 , 等 . 高速钢的生产和质量控制技术 [J]. 上海金属 , 2022 , 44 ( 2 ): 8 - 14+23 .
徐桂丽 , 黄鹏 , 孙溪 , 等 . 高速钢制备和热处理工艺的研究现状及发展趋势 [J]. 中国材料进展 , 2020 , 39 ( 1 ): 70 - 77 .
黄进峰 , 张程 , 连勇 , 等 . 两种制备工艺对含铌高速钢组织性能的影响 [J]. 材料热处理学报 , 2014 , 35 ( 8 ): 130 - 135 .
李荣 , 程光辉 , 郭江 . 热处理对喷射成形GCrl5轴承钢组织和性能的影响 [J]. 特殊钢 , 2016 , 37 ( 4 ): 49 - 51 .
樊文军 , 张胤 , 韩翠珍 . GCr15钢喷射成形沉积坯孔隙形成及致密度的分析 [J]. 特殊钢 , 2012 , 33 ( 1 ): 1 - 4 .
汪杰 , 魏宽 , 徐轶 , 等 . 喷射成形技术在高速钢中的应用 [J]. 热加工工艺 , 2015 , 44 ( 10 ): 48 - 52 .
崔成松 , 章靖国 . 喷射成形快速凝固技术制备高性能钢铁材料的研究进展(四)——喷射成形钢铁材料的工业化生产及展望 [J]. 上海金属 , 2012 , 34 ( 5 ): 47 - 50 .
吴立志 . 喷射成形高性能工具材料产业化制备技术开发 . 河北省 , 河冶科技股份有限公司, 2016-05-21 .
张海军 . 高韧高耐磨高寿命汽车锁具系列精冲模具钢开发 . 河北省 , 河冶科技股份有限公司, 2020-12-04 .
皮自强 , 路新 , 贾成厂 , 等 . 喷射成形高速钢的研究进展 [J]. 粉末冶金技术 , 2013 , 31 ( 5 ): 379 - 384 .
Ikawa Y , Itami T , Kumagai K , et al . Spray Deposition Method and Its Application to Production of Mill Rolls [J]. Tetsu-to-Hagane , 1989 , 75 ( 5 ): 766 - 773 .
Igharo M , Wood J V . Investigation of M2 High Speed Steel Produced by Osprey Process [J]. Powder Metallurgy , 1989 , 32 ( 2 ): 124 - 131 .
Ernst I C , Duh D . ESP4 and TSP4, a comparison of spray formed with powdermetallurgically produced cobalt free high-speed steel of type 6W-5Mo-4V-4Cr [J]. Journal of Materials Science , 2004 , 39 ( 22 ): 6831 - 6834 .
Mesquita R A , Barbosa C A . Spray forming high speed steel—Properties and processing [J]. Materials Science and Engineering: A , 2004 , 383 ( 1 ): 87 - 95 .
Mesquita R A , Barbosa C A . High-speed steels produced by conventional casting, spray forming and powder metallurgy [A]. Materials Science Forum [C]. Trans Tech Publications Ltd , 2005 : 244 - 250 .
Rodenburg C , Krzyzanowski M , Beynon J H , et al . Hot workability of spray-formed AISI M3:2 high-speed steel [J]. Materials Science & Engineering A , 2004 , 386 ( 1-2 ): 420 - 427 .
Zhang G Q , Yuan H , Jiao D L , et al . Microstructure evolution and mechanical properties of T15 high speed steel prepared by twin-atomiser spray forming and thermo-mechanical processing [J]. Materials Science & Engineering A , 2012 , 558 : 566 - 571 .
王和斌 . 喷射成形M3型高速钢碳化物演变规律及机理研究 [D]. 北京 : 北京科技大学 , 2015 .
卢林 . 喷射成形含铌M3型高速钢组织性能优化与应用研究 [D]. 北京 : 北京科技大学 , 2016 .
杜文华 , 张海军 , 默雄 , 等 . 喷射成形高速钢HSF8610组织与性能研究 [J]. 河北冶金 , 2021 , 310 ( 10 ): 37 - 40 .
Kjeldsteen P . Development of high alloyed tool steels using spray forming on an industrial scale [J]. Powder Metallurgy , 2003 , 46:(4), 297 - 298 .
Pi Z Q , Xin L , Yuan W , et al . Simulation of jet-flow solid fraction during spray forming [J]. International Journal of Minerals, Metallurgy and Materials , 2017 , 24 ( 6 ): 657 - 669 .
Lee E S , Park W J , Jung J , et al . Solidification microstructure and M2C carbide decomposition in a spray-formed high-speed steel [J]. Metallurgical & Materials Transactions A , 1998 , 29 : 1395 - 1404 .
Lee E S , Park W J , Baik K H , et al . Different carbide types and their effect on bend properties of a spray-formed high speed steel [J]. Scripta Materialia , 1998 , 39 ( 8 ): 1133 - 1138 .
Serna M M , Rossi J L . MC Complex carbide in AISI M2 High-speed Steel [J]. Materials Letters , 2009 , 63 ( 8 ): 691 - 693 .
Hanlon D N , Rainforth W M , Sellars C M . The rolling/sliding wear response of conventionally processed and spray formed high chromium content cast iron at ambient and elevated temperature [J]. Wear , 2003 , 255 : 956 - 966 .
刘继浩 , 周健 , 武会宾 , 等 . 喷射成形M3高速钢偏析成因及凝固机理 [J]. 金属学报 , 2023 , 59 ( 5 ): 599 - 610 .
Ernst I C , Duh D . Properties of cold-work tool steel X155CrVMo12-1 produced via spray forming and conventional ingot casting [J]. Journal of Materials Science , 2004 , 39 ( 22 ) : 6835 - 6838 .
Schulz A , Matthaei-Schulz E , Spangel S , et al . Analysis of spray formed tool steels [J]. Materialwiss. Werkst. , 2003 , 34 ( 5 ) : 478 - 483 .
Schruff I , Schüler V , Spiegelhauer C . Advanced tool steels pro‐ duced via spray forming [A]. Proceedings of the 6 th International Tooling Conference [C]. Sweden , 2002 : 1159
Sandberg O , Jonson L . New generation of tool steels made by spray forming [A]. In: Proceedings of the 6 th International Tooling Conference . The Use of Tool Steels : Experience and Research [C]. Karlstad: Karlstad University , 2002 : 2 .
李栋 , 孙宗林 , 辛栋梅 , 等 . 喷射成形与传统熔炼D2组织性能对比研究 [J]. 河北冶金 , 2015 , 235 ( 7 ): 19 - 22 .
米永旺 , 李惠 , 张巍 , 等 . 喷射成形耐蚀耐磨钢HSF340组织与性能研究 [J]. 河北冶金 , 2017 , 259 ( 7 ): 6 - 9+32 .
康少付 , 刘允中 . 喷射成形高合金工具钢微动干摩擦磨损性能研究 [J]. 热加工工艺 , 2013 , 42 ( 24 ): 127 - 130 .
颜飞 . 喷射成形高合金Vanadis4冷作模具钢的组织与性能研究 [D]. 上海 : 上海交通大学 , 2007 .
刘继浩 , 迟宏宵 , 武会宾 , 等 . 喷射成形M3高速钢热处理过程中组织的演变和硬度偏低问题 [J/OL]. 材料研究学报 : 1 - 11 . DOI 10.11901/1005.3093.2022.493.
0
浏览量
2
下载量
0
CSCD
0
CNKI被引量
关联资源
相关文章
相关作者
相关机构
京公网安备11010802024621