张笑龙,冯亮花.炉气对200 t转炉五孔氧枪超音速射流特性影响[J].特殊钢,2026,47(02):32-40.
Zhang Xiaolong,Feng Lianghua.Effects of Furnace Atmosphere on Supersonic Jet Characteristics of a Five-Nozzle Oxygen Lance in a 200-ton Converter[J].Special Steel,2026,47(02):32-40.
张笑龙,冯亮花.炉气对200 t转炉五孔氧枪超音速射流特性影响[J].特殊钢,2026,47(02):32-40. DOI: 10.20057/j.1003-8620.2025-00159.
Zhang Xiaolong,Feng Lianghua.Effects of Furnace Atmosphere on Supersonic Jet Characteristics of a Five-Nozzle Oxygen Lance in a 200-ton Converter[J].Special Steel,2026,47(02):32-40. DOI: 10.20057/j.1003-8620.2025-00159.
为解决转炉冶炼过程中高温与炉气变化显著影响氧枪超音速射流特性,而不同冶炼时期射流特性变化规律研究有限的问题,通过CFD数值模拟研究了不同温度下炉气成分对转炉炼钢过程中超音速氧气射流特性的影响。结果表明,相同炉气浓度下,高温(1 873 K)时氧枪射流核心区长度是常温(298 K)时的2.6倍;超音速区长度随炉气CO浓度升高而线性增长,且在高温时增长更快,CO浓度提升20%,常温时核心段长度延长0.048 m,高温时延长0.126 m;CO浓度升高增大氧气射流有效冲击面积,常温时最大提升11.6%,高温时提升3.1%。常温时有效冲击面积随枪位升高先增大后减小,而高温下则持续增大;冶炼中期较高的CO浓度和环境温度更利于减缓射流衰减并扩大有效冲击面积。
To address the issue that high temperatures and significant furnace gas variations during converter steelmaking substantially affect the characteristics of supersonic oxygen jets, while research on the changing patterns of jet characteristics across different smelting stages remains limited, the effect of furnace gas composition on supersonic oxygen jet characteristics in converter steelmaking under different temperatures was investigated through CFD numerical simulation.The results indicate that at the same furnace gas concentration, the core length of the oxygen lance jet at high temperature (1 873 K) is 2.6 times longer than at room temperature (298 K). The length of supersonic zone increases linearly with rising CO concentration in the furnace gas, with a more pronounced growth rate at elevated temperatures. A 20% increase in CO concentration extends the core length by 0.048 m at room temperature and by 0.126 m at high temperature. The increase of CO concentration enlarges the effective impact area of the oxygen jet, with a maximum increase of 11.6% at room temperature and 3.1% at high temperature. At room temperature, the effective impact area initially increases and then decreases as the lance height rises, whereas it continues to expand under high-temperature conditions. During the mid-blowing stage, higher CO concentration and ambient temperature contribute more effectively to slowing jet attenuation and expanding the effective impact area.
本刊编辑部 . 2021年全球主要国家(地区)废钢使用和进出口情况 [J]. 冶金管理 , 2022 ( 12 ): 52 - 55 .
姜周华 , 董艳伍 , 刘福斌 , 等 . 我国特种冶金产品、技术和装备的最新进展与展望 [J]. 特殊钢 , 2024 , 45 ( 4 ): 1 - 12 .
黄高见 , 韦泽洪 , 宋 欢 , 等 . 经济性Q355钢转炉冶炼实践 [J]. 特殊钢 , 2024 , 45 ( 1 ): 70 - 76 .
孙梦丽 , 刘广强 , 李艺璇 , 等 . 260 t转炉用双角度六孔氧枪的射流特性研究 [J]. 特殊钢 , 2022 , 43 ( 6 ): 73 - 78 .
王 玺 , 刘广强 , 韩 鹏 , 等 . 260 t转炉用五孔旋流氧枪的数值模拟 [J]. 特殊钢 , 2021 , 42 ( 1 ): 20 - 24 .
杨国军 . 转炉炼钢二级喷射氧枪的研究与开发 [D]. 南昌 : 南昌大学 , 2007 .
刘金鑫 . 转炉内气液界面相互作用及液滴喷溅行为研究 [D]. 沈阳 : 东北大学 , 2021 .
吴凤林 . 氧枪射流的一些研究结果 [J]. 冶金能源 , 1989 , 8 ( 3 ): 47 - 52 .
Hu S Y , Zhu R , Dong K , et al . Effect of oxygen flow rate and temperature on supersonic jet characteristics and fluid flow in an EAF molten bath [J]. Canadian Metallurgical Quarterly , 2018 , 57 ( 2 ): 219 - 234 .
赵 飞 , 张延玲 , 朱 荣 , 等 . 预热温度对超音速氧气射流特性影响的数值模拟研究 [J]. 有色金属科学与工程 , 2014 , 5 ( 6 ): 34 - 37 .
包丽明 , 刘 坤 , 吕国成 . 超音速氧枪射流特性的数值模拟 [J]. 特殊钢 , 2014 , 35 ( 4 ): 1 - 4 .
赵 飞 , 张延玲 , 朱 荣 , 等 . 环境压力对超音速氧气射流特性影响的数值模拟 [J]. 中国冶金 , 2014 , 24 ( 9 ): 22 - 25 .
Yang L Z , Yang Z S , Wei G S , et al . Influence of ambient and oxygen temperatures on fluid flow characteristics considering swirl-type supersonic oxygen jets [J]. ISIJ International , 2019 , 59 ( 12 ): 2272 - 2282 .
陈双平 , 吕 明 , 郝翊杰 , 等 . 基于环境温度的转炉旋流氧枪射流分析 [J]. 中国冶金 , 2024 , 34 ( 1 ): 18 - 26 .
Sumi I , Kishimoto Y , Kikuchi Y , et al . Effect of high-temperature field on supersonic oxygen jet behavior [J]. ISIJ International , 2006 , 46 ( 9 ): 1312 - 1317 .
Alam M , Naser J , Brooks G . Computational fluid dynamics simulation of supersonic oxygen jet behavior at steelmaking temperature [J]. Metallurgical and Materials Transactions B , 2010 , 41 ( 3 ): 636 - 645 .
Lebon G S B , Patel M K , Djambazov G , et al . Mathematical modelling of a compressible oxygen jet entering a hot environment using a pressure-based finite volume code [J]. Computers & Fluids , 2012 , 59 ( none ): 91 - 100 .
李子亮 , 苍大强 , 倪松明 . 转炉氧枪超音速射流特性的数值模拟 [J]. 工业炉 , 2016 , 38 ( 5 ): 6 - 10 .
胡绍岩 , 朱 荣 , 董 凯 . 炼钢温度下复吹转炉流场的数值模拟研究 [J]. 工程科学学报 , 2018 , 40 ( S1 ): 108 - 115 .
Li M M , Li Q , Kuang S B , et al . Coalescence characteristics of supersonic jets from multi-nozzle oxygen lance in steelmaking BOF [J]. Steel Research International , 2015 , 86 ( 12 ): 1517 - 1529 .
徐少禹 . 180 t转炉五孔氧枪的数值模拟及研究 [D]. 鞍山 : 辽宁科技大学 , 2014 .
Zhao F , Zhu R , Wang W R . Characteristics of the supersonic combustion coherent jet for electric arc furnace steelmaking [J]. Materials , 2019 , 12 ( 21 ): 3504 .
Li S , Wei X L , Yu L X . Numerical study on NO x /CO emissions in the diffusion flames of high-temperature off-gas of steelmaking converter [J]. Applied Energy , 2011 , 88 ( 4 ): 1113 - 1119 .
茹作栋 , 张英嘉 , 王春江 , 等 . 120 t转炉氧枪喷头优化及其在炼钢环境的射流特性研究 [J]. 炼钢 , 2022 , 38 ( 4 ): 21 - 27 .
Yao L J , Zhu R , Tang Y X , et al . Effect of furnace gas composition on characteristics of supersonic oxygen jets in the converter steelmaking process [J]. Materials , 2020 , 13 ( 15 ): 3353 .
Li S , Wei X L , Yu L X . Numerical simulation of off-gas formation during top-blown oxygen converter steelmaking [J]. Fuel , 2011 , 90 ( 4 ): 1350 - 1360 .
丁长江 , 刘国平 , 周 俐 . 利用炉气CO浓度曲线监控转炉造渣操作 [J]. 中国冶金 , 2007 , 17 ( 10 ): 16 - 19 .
姜伯炜 . 转炉烟气的余热回收系统能耗分析 [D]. 北京 : 华北电力大学 , 2022 .
Li Z L , Cang D Q . Numerical simulation of supersonic oxygen jets at high ambient temperature [J]. Steel Research International , 2017 , 88 ( 4 ): 1600209 .
武浩 . 转炉氧枪超音速射流行为及其与熔池相互作用的数值模拟 [D]. 沈阳 : 东北大学 , 2013 .
Asahara N , Naito K I , Kitagawa I , et al . Fundamental study on interaction between top blown jet and liquid bath [J]. Steel Research International , 2011 , 82 ( 5 ): 587 - 594 .
Liang H.K , Basic Research on Jet Characteristics of Coherent Jet Oxygen Lance with High Temperature . Master's Thesis , University of Science and Technology Liaoning , 2017 .
Launder B.E , Spalding D . B , Lectures in Mathematical Models of Turbulence (Academic Press , Cambridge , 1972 .
杨东亚 , 彭其春 , 童志博 , 等 . 210 t转炉氧枪射流性能优化与工业应用 [J]. 特殊钢 , 2023 , 44 ( 4 ): 15 - 21 .
吴凤林 , 蔡扶时 . 顶吹转炉氧枪设计 [M]. 北京 : 冶金工业出版社 , 1982 .
Tago Y , Higuchi Y . Fluid flow analysis of jets from nozzles in top blown process [J]. ISIJ International , 2003 , 43 ( 2 ): 209 - 215 .
张成德 . 150 t转炉二次燃烧氧枪技术研究 [D]. 沈阳 : 东北大学 , 2022 .
王文静 , 赵宏欣 , 潘贻芳 , 等 . 氧枪喷头射流的数值模拟 [J]. 钢铁研究学报 , 2010 , 22 ( 5 ): 7 - 10 .
杨文远 , 刘炳仁 , 朱立宪 , 等 . 转炉氧枪喷头的射流特性及其冶金效果 [J]. 钢铁研究学报 , 1995 , 7 ( 3 ): 8 - 15 .
赵 飞 , 张延玲 , 朱 荣 , 等 . 环境温度对超音速氧气射流特性影响的数值模拟 [J]. 北京科技大学学报 , 2014 , 36 ( 5 ): 669 - 673 .
0
浏览量
230
下载量
0
CSCD
0
CNKI被引量
关联资源
相关文章
相关作者
相关机构
京公网安备11010802024621