1.天津大学,天津 300354
2.天津钢管制造有限公司,天津 300301
黄永智(1987—),男,博士在读; E-mail : huangyongzhi2007@126.com
收稿:2026-03-13,
修回:2026-05-09,
录用:2026-05-12,
纸质出版:2026-11-30
移动端阅览
黄永智,高志明,吕传涛等.高性能双金属冶金复合油套管开发[J].特殊钢,2026,47(06):1-6.
Huang Yongzhi,Gao Zhiming,Lü Chuantao,et al.Research and Development of High-Performance Bimetallic Metallurgically Bonded Composite Tubing and Casing[J].Special Steel,2026,47(06):1-6.
针对我国深层、超深层及高酸性油气田开发中传统油套管腐蚀失效严重的瓶颈问题,开展了高性能双金属冶金复合油套管关键技术研究。通过创新“外层高强度抗硫低合金钢+内层耐蚀合金”材料体系,确定了外层抗硫低合金钢的关键成分(质量分数):≤0.008%P,≤0.002%S,0.50%~1.00%Cr,0.20%~0.40%Mo;以及内层20-40型镍基耐蚀合金的主要成分:20.00%~23.00%Cr,≥40.00%Ni,5.00%~8.00%Mo。开发了“电渣复合坯+控轧控冷”短流程制备技术,明确了电渣重熔过程熔速控制在5.0~6.5 kg/min、热轧初轧温度1 150~1 200 ℃、终轧温度≥900 ℃、累计变形量≥60%、淬火温度900~950 ℃与回火温度600~680 ℃的关键工艺参数。
<math id="M1"><mi>ϕ</mi></math>
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=122060240&type=
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=122060251&type=
2.03200006
2.87866688
88.9 mm×7.34 mm复合管界面剪切强度达到572~585 MPa,外层低合金钢材料的抗拉强度865~982 MPa,在模拟苛刻工况下均匀腐蚀速率≤0.003 mm/a,比行业标准低两个数量级。该成果已在高腐蚀性油气田完成工程示范,为我国深层油气安全高效开发提供了技术支撑。
Aiming at the bottleneck of severe corrosion failure of conventional casing and tubing in the development of deep, ultra-deep and high-sour oil and gas fields in China, a systematic study on key technologies of high-performance bimetallic metallurgically bonded composite OCTG was carried out. By adop
ting an innovative material system of "high-strength sour-service low alloy steel outer layer + corrosion-resistant alloy (CRA) inner layer", the critical chemical composition ranges (mass fraction) of the outer sour-service low alloy steel ( ≤ 0.008%P, ≤ 0.002%S, 0.50%-1.00%Cr, 0.20%-0.40%Mo) and the main composition of the inner 20-40 type nickel-based CRA (20.00%-23.00% Cr, ≥40.00% Ni, 5.00%-8.00% Mo) were determined. A short-process manufacturing route combining "electroslag remelting (ESR) composite billet + controlled rolling and cooling" was developed, through which the key process parameters were established: ESR melting rate controlled at 5.0-6.5 kg/min, initial hot rolling temperature of 1 150-1 200 ℃, finish rolling temperature ≥ 900 ℃, cumulative reduction ≥ 60%, quenching temperature of 900-950 ℃, and tempering temperature of 600-680 ℃. For the
<math id="M2"><mi>ϕ</mi></math>
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=122060255&type=
https://html.publish.founderss.cn/rc-pub/api/common/picture?pictureId=122060265&type=
2.03200006
2.87866688
88.9 mm×7.34 mm composite pipe, the interfacial shear strength reached 572-585 MPa, and the tensile strength of the outer low alloy steel was 865-982 MPa. Under simulated harsh service conditions, the uniform corrosion rate was ≤ 0.003 mm/a, which was two orders of magnitude lower than the industry standard. This achievement has been demonstrated in engineering applications in highly corrosive oil and gas fields, providing technical support for the safe and efficient development of deep oil and gas resources in China.
张 智 , 蔡 楠 , 赵苑瑾 , 等 . 四川盆地超深高含硫气田井下管柱完整性设计理念与方法 [J]. 天然气工业 , 2023 , 43 ( 4 ): 148 - 156 .
胡 勇 , 惠 栋 , 杜 强 , 等 . 四川盆地中坝气田雷三气藏高效开发及其对中国高含硫气藏开采的意义 [J]. 天然气工业 , 2024 , 44 ( 11 ): 24 - 36 .
赵密锋 , 付安庆 , 秦宏德 , 等 . 高温高压气井管柱腐蚀现状及未来研究展望 [J]. 表面技术 , 2018 , 47 ( 6 ): 44 - 50 .
Carneiro R A , Ratnapuli R C , de Freitas Cunha Lins V . The influence of chemical composition and microstructure of API linepipe steels on hydrogen induced cracking and sulfide stress corrosion cracking [J]. Materials Science and Engineering: A , 2003 , 357 ( 1-2 ): 104 - 110 .
沈 函 , 周高阳 , 王新田 , 等 . C110级油套管钢的显微组织和晶体学特征对硫化物应力开裂的影响 [J]. 上海金属 , 2023 , 45 ( 2 ): 20 - 26 .
李效华 , 侯文芝 , 吕传涛 , 等 . 冶金复合油套管技术的研究进展 [J]. 钢管 , 2024 , 53 ( 4 ): 11 - 21 .
杜心康 , 王建江 , 赵忠民 , 等 . 重力分离SHS陶瓷内衬复合管界面现象 [J]. 复合材料学报 , 2001 , 18 ( 4 ): 72 - 75 .
唐 科 , 王秀敏 , 彭 俊 , 等 . 稠油热采井用110SH-1钢级热采套管的开发 [J]. 特殊钢 , 2020 , 41 ( 4 ): 43 - 47 .
吕国成 , 包丽明 , 朱金禄 , 等 . Nb-Ti微合金化含铬J55石油套管用钢的生产实践 [J]. 特殊钢 , 2015 , 36 ( 4 ): 28 - 30 .
张玉海 , 王永然 . 石油套管钢Φ150~Φ200 mm连铸圆坯的质量控制 [J]. 特殊钢 , 2013 , 34 ( 3 ): 42 - 44 .
武利平 , 智建国 , 刘 青 , 等 . 套管TG22热轧钢带研究及产业化 [J]. 特殊钢 , 2020 , 41 ( 1 ): 21 - 23 .
Baghaei M H , Faraji G . Punch plastic deformation pipe cladding (PPDPC) as a novel tube cladding method [J]. Journal of Advanced Materials and Processing , 2016 , 4 : 21 - 28 .
KleverR F J . On the mechanics of premium connections in casing and tubing [C]. SPE Annual Technical Conference and Exhibition. Society of Petroleum Engineers , 1992 . SPE-24692-MS.
API Speccificatio 5CT. Specification for casing and tubing [S]. 10 th ed. Washington : American Petroleum Institute , 2018 incorporating errata 3, 2020 .
NACE International . NACE TM0177-2016 laboratory testing of metals for resistance to sulfide stress cracking and stress corrosion cracking in H2S environments [S]. Houston : NACE International , 2016 .
Jiang Z , ZhangY , Wang L , et al . Corrosion behavior of stainless steel cladding layer in CO 2 -H 2 S-Cl⁻ environment [J]. Corrosion Science , 2021 , 187 : 109472 .
Wang H , Zhang Z , Chen S , et al . Advanced manufacturing technologies for corrosion resistant alloy-clad OCTG for extreme sour service [C]. SPE Annual Technical Conference and Exhibition , Houston, Texas, USA , October 3-5 , 2022 . SPE-200981.
0
浏览量
0
下载量
0
CSCD
0
CNKI被引量
关联资源
相关文章
相关作者
相关机构
京公网安备11010802024621