ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2006, Vol. 27 ›› Issue (2): 31-33.

• 试验研究 • 上一篇    下一篇

重钢85t复吹转炉的水模型试验

鱼洋洋1,唐 萍1,周 亮1,龙贻菊2,陈文满2,梁 庆2,安昌遐2   

  1. 1. 重庆大学材料科学与工程学院,重庆 400030;
    2. 重庆钢铁公司炼钢厂,重庆 400030;
  • 收稿日期:2005-11-01 出版日期:2006-04-01 发布日期:2023-03-02
  • 作者简介:鱼洋洋(1981-),男,硕士研究生,从事复吹转炉工艺参数优化和底吹气体对熔池搅拌的数值模拟研究。

Water Modelling for a 85 t Top-Bottom Combined Blown Converter at Chongqing Steel

Yu Yangyang1 , Tang Ping1 , Zhou Liang1 , Long Yiju2 , Chen Wenman2 , Liang Qing2 , An Changxia2   

  1. 1. College of Materials Science and Engineering,Chongqing University,Chongqing 400030;
    2. Steelmaking Plant,Chongqing Iron and Steel Company, Chongqing 400030;
  • Received:2005-11-01 Published:2006-04-01 Online:2023-03-02

摘要: 通过重钢85 t复吹转炉1∶8的水模型,试验研究了顶枪枪位、底吹流量对转炉熔池混匀时间、炉口喷溅量、冲击深度和液面扰动的影响。实验表明,模型获得最大搅拌能的顶枪枪位为50~100 mm;枪位在90~110 mm时,由射流冲击引起的物理喷溅量达到最大值。建立了重钢85 t转炉复吹工艺参数:冶炼前期顶枪枪位为1600~1760 mm,底吹流量240~350 m3/h;中期两参数分别为1100~1300 mm和160~200 m3/h,后期两参数分别为1040~1120 mm和200~350 m3/h。

关键词: 复吹转炉, 水模型, 混匀时期, 喷溅量, 液面扰动

Abstract: The effect of top lance level and bottom blowing flowrate on mixed time in bath,mouth spraying,penetration depth in steel and liquid surface fluctuation have been studied by 1:8 water modelling of a 85 t top-bottom combined blown converter at Chongqing Steel. The test results showed that maximum stirring energy was obtained as the top lance level was at 50~100 mm and the spraying amount caused by top lance jet penetration was up to maximum as the top lance level was at 90~110 mm.The top-bottom blown parameters for the 85 t converter at Chongqing Steel has been established that in primary phase of melting the top lance level is 1600~1760 mm and the bottom blowing flowrate is 240~350 m³/h; in second phase both parameters are 1100~1300 mm and 160~200 m³/h respectively; and in later phase both are 1040 ~ 1120 mm and 200~350 m³/h.

Key words: Top-Bottom Combined Blown Converter, Water Modelling, Mixed Time, Spraying Amount, Liquid Surface Fluctuation