Effect of Finished Rolling Cooling Rate on Structure of Microalloy Non Quenched-Tempered Steel 34Mn2VN

Zhang  Yusheng1,2,Liu  Yazheng1,Liu  Zhao3,Qiao  Aiyun2,Li  Xiao2,Jing  Yinong2   

  1. 1  School  of Materials  Science  and  Engineering,University  of Science  and  Technology,Beijing  100083;
    2  Seamless  Steel  Tube  Plant,Baotou  Iron  and  Steel(Group)Co  Ltd,Baotou  014040;
    3  Department  of Machinery  and  Electricity,Hebei  University  of Engineering,Handan  056038
  • Received:2006-05-30 Published:2006-11-01 Online:2023-03-02

摘要: 用Gleeble-1500热模拟试验机研究了非调质钢34Mn2VN(%:0.30~0.34C、1.20~1.70Mn、0.014~0.018N、0.07~0.12V)在950℃、平均应变速率2s-1、应变15%后以0.1~45℃/s不同冷却速率下冷却的动态CCT曲线和组织转变。结果得出,当冷却速率控制在0.8~2.0℃/s时所得到细小的铁素体和少量贝氏体组织,具有较高的冲击韧性。生产应用表明,采用该冷却速率生产Φ139.7×7.7(mm)和Φ114.0×6.4(mm)管材的冲击功为47.8~50.9J。

关键词: 非调质钢34Mn2VN,  , 动态CCT 曲线, 组织, 冲击韧性

Abstract: Dynamic  continuous  cooling  transformation(CCT)curves  and  structure  transition  of  non  quenched-tempered     steel     34Mn2VN(0.30~0.34C,1.20~1.70Mn,0.014~0.018N,0.07~0. 12V)at  950℃  with  average  strain rate 2 s-¹and  15% strain, then cooling with 0.1~45 ℃/s different rate have been studied by Cleeble-1500 thermal simulation  machine.  The  results  obtained  that  as  cooling  rate  was  controlled  within  0.8~2.0  ℃/s,the  fine  ferrite  and  minor bainite structure was obtained, it had higher impact toughness. Commercial production application showed that the impact energy    of φ139.7×7.7(mm) and φ114.0×6.4(mm) steel    tubes    produced    with    that    cooling    rate    was    47.8~50.9    J.

Key words: Non , Quenched-Tempered , Steel , 34Mn2VN,Dynamic , CCT , Curves,Structure,Impact , Toughness