ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2007, Vol. 28 ›› Issue (6): 13-15.

• 试验研究 • 上一篇    下一篇

Ti-V-Nb微合金管线钢焊缝及热影响区中第二相粒子

耿相军1,陈茂爱2   

  1. 1山东交通学院,济南250023;
    2山东大学材料液态结构及其遗传性教育部重点试验室,济南250014
  • 收稿日期:2007-05-11 出版日期:2007-12-01 发布日期:2022-12-27
  • 作者简介:耿相军(1964-),女,讲师,1987年山东工业大学毕业,金属材料与热处理研究。
  • 基金资助:
    山东省科学技术发展计划资助项目(2006GG3204017)

Second Phase Particles in CGHAZ and Weld of Ti-V-Nb Microalloyed Pipeline Steel

Geng Xiangjun1, Chen Maoai2   

  1. 1  Shandong  Jiaotong  University,Jinan  250023;
    2  Key  Laboratory  of Liquid  Structure  and Heredity   of  Materials,Ministry   of  Education,Shandong   University,Jinan   250014
  • Received:2007-05-11 Published:2007-12-01 Online:2022-12-27

摘要: 利用萃取复型技术研究了Ti-V-Nb微合金钢(%:0.08C、1.29Mn、0.02Ti、0.04V、0.04Nb)模拟粗晶热影响区及焊缝(H08C焊丝%:0.06C、1.44Mn、0.24Mo、0.04Ti、0.01V)第二相粒子。结果表明,母材大部分第二相粒子≤30nm,平均尺寸19.70nm;焊接粗晶区仍残留较多的碳氮化合物粒子,粒子平均尺寸增大至42.78nm,粒子由母材中不规则形状变为方形,粒子Ti含量显著提高。焊缝中绝大部分碳氮化合物粒子发生溶解,熔池中生成的TiO与熔池中其他脱氧和脱硫产物结合成尺寸较大的夹杂物,在焊缝中未发现含Nb、V的夹杂物和第二相粒子。

关键词: Ti-V-Nb微合金钢, 第二相粒子, 焊缝, 粗晶热影响区

Abstract: The     second    phase    particles    in     simulated    weld(H08C    weld    wire-0.06C,1.44Mn,0.24Mo,0.04Ti,  0.01V)and     coarse     grained     heat     affected     zone(CGHAZ)of     Ti-V-Nb     microalloyed     steel(0.08C,1.29Mn,0.02Ti, 0.04V,0.04Nb)have  been  studied  by  using  carbon  extraction  replica  technique.Results  showed  that  size  of  most  second phase particles in parent metal was ≤30 nm with average  size  19.70 nm; there was a lot of residual carbo-nitride particles in CGHAZ of which the average size increased to42.78 nm,and the shape of residual particles changed from irregular morphology in parent metal to cubic in CGHAZ in which the Ti content obviously increased; and most of carbo-nitride particles in weld dissolved,the TiO formed in bath combined with other deoxidising and desulphurizing products to form large scale inclusions  and  the  inclusions  and  second particles  containing Nb,V  didn't  find  out  in  weld.

Key words: Ti-V-Nb Microalloying Steel,Second Phase Particles,Weld,CCHAZ