Development and Application Prospects for Hot Rolled Steel Sheet Piles
Ren Anchao1,2, Zhou Guifeng1,2, Ji Yu1, Zhu Min1
1 Research and Development Institute, Wuhan Iron and Steel ( Group) Corp, Wuhan 430080;
2 Institue of Material Science and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081
Ren Anchao, Zhou Guifeng, Ji Yu, Zhu Min. Development and Application Prospects for Hot Rolled Steel Sheet Piles[J]. Special Steel, 2009, 30(1): 22-24.