[1] 李鹤林.油气输送钢管的发展动向与展望.焊管,2004,27(6):1
[2] Okaguchi S.Development and Mechanical Properties of X120 Line- pipe.International Journal of Offshore and Polar Engineering,2004, 14(1):14
[3] Asahi H,Hara T.Development of Plate and Seam Welding Technology for X120 Linepipe.International Joural of Offshore and Ploar Engi- neering,2004,14(1):34
[4] Hans-Georg Hillenbrand.Development of High Strength Material and Pipe Production Technology for Crade X120 Line Pipe.Proceedings of IPC 2004 International Pipeline Conference.Calgary,Canada,2004
[5] 王路兵,武会宾,任 毅,等.X120级管线钢DQ-T工艺试验研究.金属热处理,2007,32(10):44
[6] Hans-Georg Hillenbrand,Andreas Liessem, Karin Biermann,et al. De- velopment and Production of Linepipe Steels in Grade X100 and X120.In: Seminar Forum of X100/X120 Grade High Performance Pipe Steels. Beijing,2005
[7] Mauro Pontremoli.A New Generation of Ultra High Strength X100/ X120 Pipelines.The Proceedings of the International Offshore and Po- lar Engineering Conference. USA,2005,15:31
[8] Shuji Okaguchi.Production and Development of Linepipe Steel in Grade X100 and X120.Report of Seminar Forum of X100/X120 Grade High Performance Pipe Steel. China,Beijing,2005
[9] Zajac S,Schwinn V,Tacke K H.Characterization and Quantification of Complex Baintic Microstructure in High and Ultrahigh Strength Line- pipe Steels.Materials Science Forum, China,2005,500:387
[10] Doug Fairchild.X120 Pipeline Development for Long Distance Gas Transmission Lines. Report of Seminar for use of X100/X120 Grade High Performance Pipe Steel,China,Beijing,2005
[11] Pontremoli M.高性能X100-X120管线钢开发的冶金和技术挑战.世界钢铁,2004(5):35
[12] 郑 磊,傅俊岩.高等级管线钢的发展现状.钢铁,2006,41(10):1
[13] Hara T,Asahi H,Uemori R,et al.Role of Combined Addition of Nio-bium and Boron and of Molybdenum and Boron on Hardnenability in Low Carbon Steels.ISIJ Int,2004,44(8):1431
[14] 魏伟,单以银,杨柯,等.添加Mo-B对超高强度管线钢相变组织的影响.金属学报,2007,43(9):943
[15] Hirosuke Inagaki,Masayuki Tannimura,Iwao Matsushima,et al. Effect of Cu of the Hydrogen Induced Cracking of the Pipeline Steel. Transactions ISIJ,1978,18(3):149
[16] Asahi H,Hara T.Development of Plate and Seam Welding Technolo- gy for X120 Linepipe.International Journal of Offshore and Polar En- gineering,2004,14(1):19
[17] Matlock DK,Brautigam V E,SpeerJG.Application of the Quenching and Partitioning(Q & P)Process to a Medium-Carbon,High-Si Micro-Alloyed Bar Steel. Materials Science Forum,2003,426-432:
1089
[18] SpeerJG,Rizo F C,Matlock D K,et al. The“Quenching and Parti- tioning”Process:Background and Recent Pprogress.Materials Re- searh,2005,8(4):417
[19] SpeerJG,Matlock D K,De Cooman B C,et al.Carbon Partitioning into Austenite After M Artensite Transformation.Acta Materialia, 2003,51(9):2611
[20] 江海涛,唐 获,米振莉.汽车用先进高强度钢的开发及应用进 展.钢铁研究学报,2007,19(8):1
[21] Seung Chan Hong,Jae Cheon Ahn,Sang Yong Nam,et al. Mechani- cal Properties of High-Si Plate Steel Produced by the Quenching and Partitioning Process. Metals and Materials International,2007,13(6):439
|