热处理对耐热钢X12CrMoWVNbN10-1-1力学性能的影响

杨 钢1, 刘军和2,  宋玺玉2, 李许明2, 马凤春2   

  1. 1 钢铁研究总院,北京100081;2沈阳黎明发动机有限公司,沈阳110043
  • 收稿日期:2010-01-13 出版日期:2010-08-01 发布日期:2022-11-20
  • 作者简介:杨 钢(1963-),男,博士,教授级高级工程师,1984年浙江大学毕业,耐热钢及合金开发和研究。
  • 基金资助:
    国 家 高 技 术 研 究 发 展 计 划 项 目 资 助 (8 6 3) (2009AA03Z509)

Effect of Heat Treatment on Mechanical Properties of Heat Resistant Steel X12CrMoWVNbN10-1-1

Yang   Gang1, Liu   Junhe2, Song   Xiyu2, Li   Xuming2, Ma   Fengchun2   

  1. 1 Central Iron and Steel Research Institute, Beijing 100081.
    2 Shenyang Liming Engine Manufacturing Co, Shenyang 110043
  • Received:2010-01-13 Published:2010-08-01 Online:2022-11-20

摘要: 研究了淬火温度1025~1125℃+570℃4 h空冷+720℃2 h空冷和1050~1075℃淬火后二次回火温度680~780℃对马氏体耐热钢X12CrMoWVNbN10-1-1(%:0.11C、10.28Cr、0.77Ni、1.0Mo、0.96W、0.18V、0.04Nb、0.053N)力学性能的影响。结果表明,随淬火温度的提高,钢的强度增加,塑性变化不大,但冲击韧性显著下降。随回火温度的提高,强度下降、塑性、韧性增加。该钢优化的热处理工艺为:1 050~1 075℃1~2 h油冷+570℃4 h空冷+715~725℃2 h空冷。

Abstract: The    effect    of    quenching    temperature1025~1125℃+570℃4    h    air    cooling    +    720    ℃    2    h    air    cooling  and    secondary    tempering    temperature    680~780    ℃    after1050~1075    ℃    quenching    on    mechanical    properties    of    martensite  heat                     resistant                     steel                     X12CrMoWVNbN10- 1- 1(%:0. 11C,10.28Cr,0.77Ni,1.0Mo,0.96W,0. 18V,0.04Nb,0.053N)  has    been    studied.    Results    show    that    with    increasing    quenching    temperature,the    strength    of   steel    increases,of   which    the  plasticity    has    no    appreciable    change,but    the    impact    toughness    obviously    decreases;    with    increasing    tempering    temperature,  the   strength   of   steel   decreases,while   the   plasticity   and   impact   toughness   of   steel   increase.   The   optimizing   heat   treatment   of the     steel     is1050~1075℃1~2h     oil     cooling     +570℃4h     air     cooling     +715~725     ℃     2     h     air     cooling.