[1] 朱宝田,周荣灿.进一步提高超超临界机组蒸汽参数应注意的问题[J].中国电机工程学报,2OO9,29(S1 ):95-100.
[2] Gaylord D S,Howard W S. Introduction of an Advanced Superheater Alloy for Coal-fired Boiers [C]. Nace Corrosion, 2000, Paper No. 00256.
[3] Castello P,Guttmann V,Farr N,et al. Laboratory-simulated Fuel-ash Corrosion of Superheater Tubes in Coal-fired Ultra-supercritical-boilers [J]. Materials and Corrosion ,2000,51 :786-790.
[4] Zhao S Q,Dong J X,Xie X S,et al. Thermal Stability Study on a New Ni-Cr-Co-Mo-Nb-Ti-Al Superalloy [C]. The Tenth International Symposium on Superalloys ,2004 ;63-72.
[5] Zhao J C, Ravikumar V, Beltran A M. Phase Pecipitation and Pase Sability in Nimonic 263 [J]. Metallurgical and Materials Transactions A,2001,32A:1271-1282.
[6] 张红军,周荣灿,侯淑芳,等.先进超超临界机组用候选材料Alloy 263的组织稳定性[J].动力工程学报,2011,31 (12):969- 973.
[7] 赵双群,谢锡善.超超临界锅炉过热管材的高温组织稳定性及其改进研究[J].材料导报,2004,18(8):131-133.
[8] Cowen C J,Danielson P E,Jablonski P D. The Microstructural Evolution of Inconel Alloy 740 during Solution Treatment, Aging, and Exposure at 760° [J]. Journal of Materials Engineering and Performance,2011,20(6) : 1078-1083.
[9] Zhao S Q,Jiang Y,Dong J X,et al. Experimental Investigation and Thermodynamic Calculation on Phase Preciptiation of Inconel 740 [J]. Acta Metallurgica Sinica ( English Letters) ,2006,19(6) :425- 431.
[10] Evans N D,Maziasz P J,Swindeman R W,et al. Microstructure and Phase Stability in Inconel Alloy 740 during Creep [J]. Scripta Materieilia,2004,51:503-507.
[11] 张红军,周荣灿,侯淑芳,等.先进超超临界机组用Inconel 740 合金的组织稳定性研究[J].中国电机工程学报,2011,31(8): 108-113.
[12] 郭建亭.高温合金材料学(上)[M].北京:科学出版社,2008:128-129.
[13] 祝群喜,关 华.铌对镍基合金蠕变性能的影响[J].物理测试,2005,23(3):33-34.
|