冷轧压下率和再结晶退火温度对Ti-IF钢织构和成型性能的影响

罗海燕1,肖欢2,赵刚2,余冲2,孙宏云2,魏俊杰2,樊雷3   

  1. 1广西冶金研究院,南宁530023 ;
    2武汉科技大学材料加工工程系,武汉430081:
    3广西柳州钢铁(集团)公司,柳州545002
  • 收稿日期:2013-06-14 出版日期:2013-12-01 发布日期:2022-09-08
  • 作者简介:罗海燕(1962-),女,硕士,高级工程师,1987年武汉科技大学(原武汉钢铁学院)毕业,材料成型过程控制、材料的组织及性能控制研究。
  • 基金资助:
    2012年国家自然科学基金项目“基于CSP热轧带钢生产HiB取向硅钢组织演变和织构形成机理的研究"(51274155)

Influence of Cold Rolling Reduction and Annealing Temperature on Texture and Formability of Ti-IF Steel

Luo Haiyan1, Xiao Huan2, Zhao Gang2, Yu Chong2, Sun Hongyun2, Wei Junjie2 , Fan Lei3   

  1. 1 Guangxi Metallurgy Research Institute, Nanning 530023;
    2 Department of Materials Processing Engineering, Wuhan University of Science and Technology, Wuhan 430081 ;
    3 Guangxi Liuzhou Iron and Steel Co, Liuzhou 545002
  • Received:2013-06-14 Published:2013-12-01 Online:2022-09-08

摘要: 采用背散射衍射技术(EBSD)研究了3.13 mm热轧板的冷轧压下量(65%~80%)和再结晶退火温度(660~780℃)对0.64~1.10 mm Ti-IF钢冷轧板(/%:0.02C、0.01Si、0.10Mn、0.013P、0.011S、0.064 Ti、0.028Al、0.002 0N)的织构和成型性能应变硬化指数(n)、塑性应变比(r)的影响。结果表明,Ti-IF钢冷轧板在冷轧压下率为75%时{111}织构含量最大,成型性能最佳;在740℃以下再结晶退火时材料{111}<110>织构含量高,高于740℃时材料{111}<112>织构含量高;在660~780℃再结晶退火随温度增高,材料{111}织构含量增加,成型性能提高。

关键词: Ti-IF钢 , 冷轧板, 压下率 , 退火温度 , 织构 , 成型性

Abstract: The influence of cold rolling reduction (65% ~ 80% ) of 3. 13 mm hot rolled plate and recrystallization annealing temperature (660 ~ 780 °C ) on texture and formability-train-hardening exponent (n) and plastic stain ratio (r) of 0.64~1. 10 mm cold rolled sheet of Ti-IF steel (/% : 0.02C, 0.01 Si, 0. 10Mn, 0.013P, 0.011S, 0.064Ti, 0. 028Al, 0.002 0N) has been studied by electro backscattering diffraction method. Results show that with cold rolling reduction 75% the {111} texture content in Ti-IF cold rolled sheet is highest and the formability is optimum ; with recrystallization annealing at ≤740 ℃ the {111} < 110 > texture content in material is high and with annealing at more than 740 ℃ the  {111} < 112 > texture content in material is high ; and as recrystallization annealing at 660 ~780 °C , with rising annealing temperature the {111} texture content in material increases and the formability of material also increases.