ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2013, Vol. 34 ›› Issue (6): 56-58.

• 组织和性能 • 上一篇    下一篇

氮对316LN奥氏体不锈钢力学性能和耐蚀性的影响

陈海涛1,罗毅军2   

  1. 1钢铁研究总院特殊钢研究所,北京100081 ;
    2中国核动力研究设计院设计所,成都610041
  • 收稿日期:2013-06-17 出版日期:2013-12-01 发布日期:2022-09-08
  • 作者简介:陈海涛(1978-),男,硕士研究生(钢铁研究总院),高级工程师,2007年北京科技大学(本科)毕业,不锈钢及耐蚀合金 材料研究。
  • 基金资助:
    国家重大科技专项“核电站关键材料性能研究”课 题(No. 2011ZX06004-016)资助

Effect of Nitrogen on Mechanical Properties and Corrosion Resistance of Austenite Stainless Steel 316LN

Chen Haitao1 , Luo Yijun2   

  1. 1 Institute for Special Steels, Central of Iron and Steel Institute, Beijing 100081 ;
    2 Design Institute, Nuclear Power Institute of China, Chengdu 610041
  • Received:2013-06-17 Published:2013-12-01 Online:2022-09-08

摘要: 试验用316LN钢(/%:0.015C、0.65Si、0.90Mn、17.3Cr、12.8 Ni、2.6Mo、0.018~0.200N)由50 kg真空感应炉冶炼,破真空后加入氮化铬铁,铸锭锻成Φ20 mm棒材和热轧成4 mm板材,并分别经1 100℃30 min和10min水淬固溶处理。研究结果表明,316LN不锈钢每增加0.010%的氮,抗拉强度提高9 MPa,屈服强度提高7 MPa;伸长率降低0.55%,氮含量对断面收缩率没有影响,约保持在72.5%;氮强烈提高316LN不锈钢的耐点腐蚀性能,每增加0.010%的氮,其点蚀击穿电位提高7 mV;添加适宜的氮(0.079%N),可以改善316LN不锈钢的耐晶间腐蚀性能,过高的氮含量(超过0.120%N)对晶间腐蚀性能有害。

关键词: 氮, 316LN奥氏体不锈钢, 拉伸性能, 点腐蚀, 晶间腐蚀

Abstract: The steel 316LN for test (/% : 0.015C, 0. 65Si, 0. 90Mn, 17.3Cr, 12.8Ni, 2. 6Mo, 0. 018 ~ 0. 200N) is melted by a 50 kg vacuum induction furnace, adding chromium nitride in atmosphere after vacuum refining. The ingot is forged to Φ20 mm bar and hot-rolled to 4 mm sheet, then solid-solution-treated respectively at 1 100 for 30 min and 10 min, water quenching. Research results show that with increasing every 0. 010%N in stainless steel 316LN, the steel tensile strength and yield strength increase respectively by 9 MPa and 7 MPa, but the steel elongation decreases by 0. 55% , while the nitrogen content in steel on steel reduction of area has no influence, it keeps to about 72. 5% ; the nitrogen strongly improves the pitting corrosion resistance of stainless steel 316LN, with increasing every 0. 010% N, the pitting breakdown potential increases by 7 mV ; and appropriate adding nitrogen in steel (0. 079% N) is available to improve intergranular corrosion resistance of stainless steel 316LN, but excessive nitrogen content (more than 0. 120% N) is harmful to intergranular corrosion resistance of steel.