改善2Cr13马氏体不锈钢150 mm x 150 mm连铸坯表面质量的工艺实践

张迎春1,2,成国光1,钱国余1,刘敬军2,贾育华2,邸永田2   

  1. 1北京科技大学钢铁冶金新技术国家重点实验室,北京100083 ;
    2邢台钢铁有限责任公司炼钢厂,邢台054027
  • 收稿日期:2014-06-28 出版日期:2014-12-01 发布日期:2022-08-20
  • 作者简介:张迎春(1979-),男,硕士研究生(北京科技大学),2003年西安建筑科技大学(本科)毕业,不锈钢生产工艺及质量控 制。

Process Practice of Improvement on Surface Quality of 150 mm x 150 mm Casting Billet of Martensite Stainless Steel 2Cr13

Zhang Yingchun1,2, Cheng Guoguang1, Qian Guoyu1, Liu Jingjun2, Jia Yuhua2 , Di Yongtian2   

  1. 1 State Key Laboratory of Advanced Metallurgy, University of Science and Technology, Beijing 100083 ;
    2 Steelmaking Works, Xingtai Iron and Steel Co Ltd, Xingtai 054027
  • Received:2014-06-28 Published:2014-12-01 Online:2022-08-20

摘要: 2Cr13不锈钢(/%:0.160.25C,≤1.0Si,≤1.0Mn,≤0.035P,≤0.030S,12.0~14.0Cr)150 mm×150 mm铸坯生产流程为铁水预处理-50 t AOD-LF-CCM,缓冷,退火,修磨。工业性试生产结果表明,通过采用粘度(0.58±0.1)Pa·s,碱度0.95±0.01,熔点波动范围5℃的结晶器保护渣,拉速从1.3 m/min降至1.1 m/min,振幅从3 mm提高到5 mm,振动频率从139次/min减到137次/min,钢水过热度从35℃降至20~30℃,铸坯收得率达94.07%,消除了铸坯纵向凹陷和裂纹,铸坯缓冷后可直接轧制,可省去铸坯退火、修磨两道工序,降低了生产成本。

关键词: 2Cr13马氏体不锈钢 , 铁水预处理-50 t AOD-LF-CCM , 150 mm x 150 mm连铸坯 , 表面质量

Abstract: The flow sheet for production of 150 mm x 150 mm casting billet of stainless steel 2Cr13 (/% : 0. 16 ~ 0.25C, ≤1.0Si, ≤1.0Mn, ≤0.035P, ≤0,030S, 12. 0 - 14. 0Cr) is hot metal pretreatment-50 t AOD-LF-CCM, slow cooling, annealing and grinding. Commercial pilot production results show that with the technology measures including using mold powder with viscosity (0. 58 ±0. 1) Pa • s, basicity 0. 95 ± 0. 01, and melting point fluctuating extent 5 ℃ , casting speed decreasing from 1. 3 m/min to 1. 1 m/min, mold oscillation amplitude increasing from 3 mm to 5 mm, oscillation frequency decreasing from 139 times/min to 137 times/min and liquid superheating extent decreasing from 35 °C to 20 - 30 °C,the surface longitudinal depression and crack are eliminated and the yield of billet is up to 94. 07% , the low-cooled billets can direct-roll to save both procedure of billet annealing and grinding and decrease the production cost.