带过滤器63t中间包钢液流场的物理和数学模拟

赵丹婷1,2,刘爱强2,仇圣桃2,赖朝彬1   

  1. 1江西理工大学冶金与化学工程学院,赣州341000;
    2钢铁研究总院连铸中心,北京100081
  • 收稿日期:2016-07-22 出版日期:2016-12-01 发布日期:2022-07-26
  • 作者简介:赵丹婷(1991-),女,硕士研究生(江西理工大学),2014年吉林大学(本科)毕业,中间包冶金研究。

Physical and Mathematical Simulation on Flow Field of Liquid in 63t Tundish with a Filter

Zhao Danting1,2, Liu Aiqiang2, Qiu Shengtao2,Lai Chaobin1   

  1. 1 School of Metallurgical and Chemical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000;
    2 Center for Continuous Casting, Central Iron and Steel Research Institute, Beijing 100081
  • Received:2016-07-22 Published:2016-12-01 Online:2022-07-26

摘要: 通过采用几何相似比0.29:1的水模型和数学模型分别对(a)湍流抑制器和挡墙+坝(原结构),(b)湍流抑制器,挡墙+坝和过滤器,以及(c)湍流抑制器,挡墙和过滤器3种结构两流板坯连铸中间包钢液流场、温度场和夹杂物运动轨迹进行模拟研究。结果表明,原中间包结构(a)活塞区体积偏小,死区体积偏大;加入通道式钢液过滤器(b)后短路流基本消失,中间包死区减小6.83%,钢液的平均停留时间由287.04 s延长至373.76 s,有利于夹杂物的上浮去除,且过滤器的加入对钢液的温降影响不大;用钢液过滤器代替挡坝(c)后优化效果最为明显,中间包钢液平均停留时间由287.04 s延长至404.26 s,峰值时间由原来的95,4 s延长至190.8 s,死区体积由36.10%减小至8.76%。

关键词: 63t中间包, 板坯连铸, 水模型, 停留时间分布(RTD)曲线, 通道式钢液过滤器, 数值模拟

Abstract: The simulation research on liquid flow field, temperature field and inclusions moving trace in tundish for two strands slab casting with 3 kinds of structure-(a) turbulence inhibitor and wall + dam (original structure) , (b) turbulence inhibitor, wall + dam and channel filter and (c) turbulence inhibitor, wall and channel filter has been carried out by using geometric similarity 0. 29 : 1 water model and mathematical model. Results show that in tundish with original structure (a) the plug flow area is relatively small and the dead area is rather large; by adding channel liquid filter (b) the short circuit flow basically disappears, the dead volume in tundish decreases by 6. 83% and the average resident time of liquid increases from 287. 04 s to 373. 76 s, it is available to remove the inclusions from liquid and the effect of filter on drop in temperature of liquid is not obvious ; by using the filter to replace the dam (c) the effect of optimization is particularly obvious, that is the average residence time of liquid in tundish increases from 287. 04 s to 404.26 s, the peak time increases from original 95. 4 s to 190.8 s and the dead volume decreases from 36.10% to 8.76% .