精炼渣组成对31CrMoV9钢夹杂物的影响

徐泽宇,刘吉辉,何志军,丛云伶,庞清海,湛文龙   

  1. 辽宁科技大学辽宁省化学冶金重点实验室,鞍山114051
  • 收稿日期:2017-02-12 出版日期:2017-08-01 发布日期:2022-07-18
  • 作者简介:徐泽宇(1992-),男,硕士研究生,2015年辽宁科技大学(本 科)毕业,特殊钢研究。 刘吉辉(198O-),女,硕士(辽宁科技大学),讲师,特殊钢研究。
  • 基金资助:
    国家自然科学基金(51474124, 51504131, 51504132),
    辽宁省教育厅项目(L2014111),
    辽宁省 科技厅项目(2015020192)资助

Effect of Refining Slag Ingredient on Inclusions in Steel 31CrMoV9

Xu Zeyu, Liu Jihui, He Zhijun, Cong Yunling, Pang Qinghai , Zhan Wenlong   

  1. Key Lab of Liaoning Province for Chemical Metallurgy, Liaoning University of Science and Technology, Anshan 114051
  • Received:2017-02-12 Published:2017-08-01 Online:2022-07-18

摘要: 试验用31CrMoV9钢(/%:0.28~0.33C,0.30~0.35Si,0.49~0.60Mn,0.011~0.016P,0.027~0.031S,2.47~2.60Cr,0.16~0.23Mo,0.12~0.19V)由25kg感应炉熔炼,采用正交试验研究了二元碱度2.53.5不同成分精炼渣(/%:46.43~59.89CaO,15.16~23.50SiO2,10~20Al2O3,6~10MgO,2~5CaF2)对31CrMoV9钢夹杂物数量、尺寸和成分的影响。结果表明,精炼渣二元碱度和氧化铝含量对该钢夹杂物含量的影响显著;当二元碱度从2.5增加到3.5时,每0.3 mm2钢中夹杂物的平均面积从22.07μm2增至25.67μm2,增幅为16.31%;夹杂物的数量从316.67个/0.3 mm2降至255.00个/0.3 mm2,降幅为19.47%,且有利于形成复合型夹杂物。当氧化铝含量从10%增加到20%,每0.3 mm2钢中夹杂物的面积由22.57μm2增至24.28μm2,增幅为7.55%,夹杂物的数量由292.67个/0.3 mm2降至272.00个/0.3 mm2,降幅为7.06%,并易形成镁铝尖晶石类夹杂物。综合分析,当精炼渣成分为10%Al2O3、10%MgO、5%CaF2、二元碱度为3.5时精炼效果最佳。

关键词: 31CrMoV9钢, CaO-SiO2-Al2O3-MgO-CaF2系精炼渣, 碱度, Al2O3, , 夹杂物

Abstract: Tested steel 31CrMoV9 (/% : 0.28 ~0.33C, 0.30 ~0.35Si, 0.49 ~0.60Mn, 0. 011 ~0.016P, 0.027 ~ 0.031S, 2.47 ~2.60Cr, 0. 16 ~0.23Mo, 0. 12 ~0. 19V) is melted by a 25 kg induction furnace, and the effect of binary basicity 2.5 ~ 3.5 of different ingredient refining slag (/% : 46.43 - 59. 89CaO, 15.16 - 23.50Si02, 10 〜20Al2O3, 6 〜 10MgO, 2 ~5CaF2) on number, size and composition of inclusions in steel 31CrMoV9 has been studied by orthogonal experiment method. Results show that the effect of binary basicity and alumina content in refining slag on inclusion content in this steel is obvious ; as the binary basicity of slag increases from 2.5 to 3.5, for per 0.3 mm2 steel the average area of inclusions increases from 22.07 μm2 to 25.67 μm i. e. that increases by 16.31% and the number of inclusions decreases from 316.67/0.3 mm2 to 255.00/0. 3 mm2, i. e. that decreases by 19. 47% , it is available to form composite inclusions; as alumina content in slag increases from 10% to 20% , for per 0. 3 mm2 steel the area of inclusions increases from 22. 57 μm2 to 24. 28 μm2, i. e. that increases by 7. 55% and the number of inclusions decreases from 292. 67/0.3mm2 to 272.00/0.3 mm2, i. e. that decreases by 7. 06% , it is available to form aluminium-magnesium spinal inclusions. With comprehensive analysis the refining slag contained 10% Al2O3 , 10% MgO and 5% CaF2 with binary basicity 3.5 has better refining effect.