GH2907 合金 VIM + VAR 3 t 钢锭 1190℃均质化过程中Nb和Si的扩散行为

王志刚1,2,文嘉利3,杨贵新4,郑振宇2,廖凯5,韩光炜1   

  1. 1. 钢铁研究总院高温材料研究所,北京100081;
    2. 高品质特殊钢湖北省重点实验室,黄石435001;
    3. 贵州航宇科技发展股份有限公司,贵阳550081;
    4. 湖北工程职业学院,黄石435000;
    5. 黄石市产品质量监督检验所,黄石435000;
  • 收稿日期:2020-11-26 出版日期:2021-07-15 发布日期:2022-03-09
  • 作者简介:王志刚(1982-),博士生,教授级高级工程师,2005年东北大学(本科)毕业,高温合金产品及生产工艺研发。

Diffusion Behavior of Nb and Si in GH2907 Alloy VIM + VAR 3 t Ingot During Homogenization Process at 1190 ℃

Wang Zhigang1,2, Wen Jiali3, Yang Guixin4 , Zheng Zhenyu2 , Liao Kai5,Han Guangwei1   

  1. 1. Central Iron and Steel Research Institute,High Temperature Material Research Institute, Beijing, 100081 ;
    2. Hubei Key Laboratory of High Quality Special Steel,Huangshi,435001 ;
    3. Guizhou Hangyu Technology Development Co Ltd, Guiyang ,550081 ;
    4. Hubei Engineering Vocational College, Huangshi, 435000 ;
    5. Huangshi Product Quality Supervision and Inspection Institute, Huangshi 435000;
  • Received:2020-11-26 Published:2021-07-15 Online:2022-03-09

摘要: 利用光学显微镜、扫描电镜等研究了 GH2907(0.02C,38.20Ni,13.92Co,4.92Nb,1.60Ti,0.32Si)合金Φ508 mm 3 t钢锭Nb和Si在1190℃的扩散规律。研究表明,GH2907合金Φ508 mm钢锭的枝晶间距大约110μm,Nb和Si在1190℃的表观扩散系数分别为D=(0.704±0.041)× 10-14 m2/s,和D=(1.870±0.511)×10-14m2/s。理论计算表明,1190 ℃Nb扩散44.8~50.3 h,Si扩散14.0~24.5 h可使其残余偏析指数δi达到0.02。

关键词: GH2907合金, 1190℃扩散, 表观扩散系数, 偏析

Abstract: Nb and Si diffusing rule at 1 190℃ in GH2907 (0.02C,38,20Ni,13.92Co,4. 92Nb,l. 60Ti,0.32Si) alloy ϕ508 mm 3 t ingot is studied by using optical microscope, scanning electron microscope etc. Studies have shown that the dendrite spacing of the GH2907 alloy ϕ508 mm ingot is approximately 110μm, the apparent diffusion coefficients of Nb and Si at 1190℃ are respectively D = (0.704 ±0.041) X 10-14m2/s and D = (1. 870 ±0.511) x 10-14m2/s. Theoretical calculation shows that,when Nb diffuses 44.8 ~50.3 h or Si diffuses 14.0~24.5 h at 1 190℃,the residual segregation index δi will reach 0.02 respectively.