[1] 沈万林,张志成,罗小燕.60 t LF精炼终点GCrl5轴承钢中氧化物夹杂特性的研究[J].特殊钢,2018,39(1):22-27.
[2] 田超,刘剑辉,董瀚.进口与国产轴承钢夹杂物特征的对比研究[J].热加工工艺,2017,46(24):58-62.
[3] Wu H,Li Q,Wei C,et al.Study on the Behaviour of DS-Class Inclusions in Advanced Bearing Steel[J]. Metallurgical Research & Technology ,2019,116(2):223-230.
[4] ISO 4967-2013, Steel Determination of Content of Non-Metallic Inclusions Micrographic Method Using Standard Diagrams [S]. 2013 :1-3.
[5] 中华人民共和国国家质量监督检验检疫总局.GB/T18254-2016 高碳铬轴承钢[S]. 2016:7.
[6] 刘 浏.特殊钢发展新趋势与工艺创新[J].炼钢,2017,33(4):1-11.
[7] Deng Z,Zhu M. Evolution Mechanism of Non-Metallic inclusions in Al-Killed Alloyed Steel During Secondary Refining Process [J]. ISIJ International,2013,53(3) :450-458.
[8] Fujii K,Nagasaka T,Hino M. Activities of the Constituents in Spinel Solid Solution and Free Energies of Formation of MgO, MgO • Al2O3 [J]. Transactions of the Iron & Steel Institute of Japan, 2000,40,1059-1066.
[9] 黄希祜.钢铁冶金原理(第3版)[M],北京:冶金工业出版社,2002.
[10] Zhongting M A. Thermodynamic Description for Concentrated Metallic Solutions L sing Interaction Parameters [J]. Metallurgical & Materials Transactions B,2001 ,32(1) :87-103.
[11] Ohta H, Suito H. Thermodynamics of Aluminum and Manganese Deoxidation Equilibria in Fe-Ni and Fe-Cr Alloys [J]. ISIJ international ,2003,43(9) :1301-1308.
[12] Taguchi K,Hideki 0 N,Usui T,et al. Complex Deoxidation Equilibria of Molten iron by Aluminum and Calcium [J]. ISIJ International, 2005,45(11) :1572-1576.
[13] Wenjun M A,Bao Y,Wang M,et al. Effect of Mg and Ca Treatment on Behavior and Particle Size of Inclusions in Bearing Steels [J]. ISIJ International,2014,54(3) :536-542.
[14] 雷家柳,李德胜,朱航宇.基于IMCT理论的轴承钢精炼渣系碱度模型[J] .钢铁钒钛,2019,40(2) : 115-119.
[15] Yang G W,Wang X H,Huang F X,er al. Influence of Calcium Addition on Inclusions in LCAK Steel With Ultralow Sulfur Content [J]. Metallurgical & Materials Transactions B,2015 ,46( 1) : 145- 154.
[16] Verma N, Pistorius P C,Fruehan R J ,et al. Transient Inclusion Evolution During Modification of Alumina Inclusions by Calcium in Liquid Steel: Part I. Background,Experimental Techniques and Analysis Methods [ J ] . Metallurgical & Materials Transactions B, 2011,42 (4) :711-719. |