特殊钢 ›› 2022, Vol. 43 ›› Issue (1): 82-85.

• 组织和性能 • 上一篇    下一篇

38MnSiVS5 非调质钢的 CCT 曲线测定与分析

张  念1,陈章明1赵红强1,郑文超1罗时杰1,凌  鑫1赵晓丽2   

  1. 1 湖北新冶钢有限公司技术中心,黄石 435001;
    2 北京交通大学机械与电子控制工程学院,北京 100044
  • 收稿日期:2021-05-26 出版日期:2022-01-25 发布日期:2022-03-18
  • 作者简介:张 念(1989-),男,工程师,2011 年武汉科技大学(本科) 毕业,非调质钢产品开发和工艺研究。
  • 基金资助:
    国 家 “十 三 五 ” 重 点 研 发 计 划 项 目 资 助 (No. 2016YFB0300100)

Determination and Analysis of CCT Curves of Non-Quenched and Tempered Steel 38MnSiVS5

Zhang Nian1, Chen Zhangming1,Zhao Hongqiang1, Zheng Wenchao1,Luo Shijie1,Ling Xing1,Xiaoli2   

  1. 1 Technology Center, Hubei Xinyegang Steel Co Ltd, Huangshi 435001;
    2 School of Mechanical, Electronic and Control Engineering, Beijing Jiaotong University, Beijing 100044
  • Received:2021-05-26 Published:2022-01-25 Online:2022-03-18

摘要: 采用淬火膨胀仪、光学显微镜、维氏硬度计等研究了典型非调质钢38MnSiVS5(/%:0.37C,0.78Si,0.012P,0.045S,0.03Mo,0.120V,0.004Nb,0.003Ti)的显微组织和硬度。测定了其过冷奥氏体连续冷却转变(CCT)曲线。结果表明,38MnSiVS5钢的CCT曲线可分为高温转变区域、中温转变区域和低温转变区域。当冷却速度≤0.89℃/s时为全高温转变区,组织为铁素体和珠光体;当冷却速度为1.78~4.45℃/s时为高温、中温两相复合转变区,组织为铁素体、珠光体和贝氏体;当冷却速度为8.9℃/s时,为高温、中温、低温三相复合转变区,组织为铁素体、珠光体、贝氏体和马氏体;当冷却速度为17.8℃/s时,铁素体和珠光体消失,为中温、低温两相复合转变区,组织为贝氏体+马氏体;当冷却速度≥44.5℃/s时为马氏体转变区。随着冷却速度从0.06℃/s增大到44.5℃/s,38MnSiVS5钢的HV5显微硬度值由213增加至568。

关键词: 非调质钢, 38MnSiVS5,  ,  连续冷却相变,  ,  显微组织,  ,  显微硬度,  ,  CCT 曲线

Abstract: The microstructure and micro-hardness of typical non-quenched and tempered steel 38MnSiVS5 ( /% : 0. 37C,0. 78Si,0. 012P,0. 045S,0. 03Mo,0. 120V,0. 004Nb,0. 003Ti) are analyzed by using thermal dilatometer, optical microscope and Vickers hardness tester. The continuous cooling transformation ( CCT ) curves of supercooled austenite are tested. The results show that the CCT curve of steel 38MnSiVS5 could be divided into high temperature transition region, middle temperature transition region and low temperature transition region. With cooling rate ≤0.89 ℃/s, the high temperature transition region is formed with microstructure ferrite and pearlite; With the cooling rate 1.78 ~4.45 ℃/s, the high temperature transition region and middle temperature compound transition region is formed with microstructure ferrite, pearlite and bainite; as the cooling rate up to 8. 9 ℃/s, the high temperature transition region, middle temperature transition region and low temperature transition region are formed with microstructure ferrite, pearlite, bainite and martensite; as the cooling rate up to 17. 8 ℃/s, the F + P structure disappears,the middle temperature transition region and low temperature transition region are formed, the microstructure is bainite and martensite; as the cooling rate ≥44.5 ℃/s, the microstructure is martensite. With the increase of cooling rate from 0. 06 to 44. 5 ℃/s, the HV5 micro-hardness number of 38MnSiVS5 steel increased from 213 to 568.