[1]欧阳德刚,王庆方,刘守堂,等.KR脱硫搅拌器的技术现状与发展方向[J].武钢技术,2005(5);58-62.
[2]张茂林,徐安军.KR法与喷吹法在铁水脱硫中应用的比较[J]. 炼钢,2009,25(5):73-77.
[3] Nakai Y,Kikuchi N,Iwasa M,et al.Development of Slag Recycling Process in Hot Metal Desulfurization with Mechanical Stirring[J] Steel Research Intenational,2009,80(10):727-732.
[4]程新德,孙江龙,周家健,等.KR法铁水脱硫的流动数值模拟分析[J].武汉科技大学学报,2015,38(5):330-335.
[5]闵昌飞,但斌斌,牛清勇,等.挡板改善KR法脱硫搅拌效果的数值分析[J].武汉科技大学学报,2020,43(5):340-345.
[6]Iou W,WangX,LiuZ,et al,Numerical Simulation of Desulfurization Bchavior in Ladle with Bottom Powder Injection [J]. ISIJ International,2018,58(11):2042-2051.
[7]王坤,刘 燕,张廷安.底吹-机械搅拌耦合铁水脱硫的模拟[J].东北大学学报(自然科学版),2018,39(6):818-822.
[8]董佳鹏,张立峰,赵艳宇,等.KR法铁水脱硫过程铁水混合现象的水模型[J].钢铁研究学报,2021,33(2):103-109.DOI:10. 13228/j.boyuan.issn1001-0963.20200117.
[9]ChoMK,ChengJ,Park JH,et al.Hot Metal Desulfurization by CaO-SiO2-CaF2-Na2O Slag Saturated with MgO [J]. ISIJ Intemational,2010,50(2):215-221.
[10] DongK,Iong WU,Liu WJ,et al.Desulfurization of CaO-Al2O₃- SiO2-TiO2 Slag System[J]. ISIJ Intemational,2014,54(10): 2248-2254.
[11] Matsui A,Uchida YI,Kikuchi N,et al.Effects of Temperature and Oxygen Potential on Removal of Sulfur from Desulfurization Slag [J].Tetsu-to-Hagane,2016,102(10):553-559.
[12]Nakai Y,SumiI,Kikuchi N,et al.Aggregation Behavior of Des- ulfurization Flux in Hot Metal Desulfurization with Mechanical Stir- ring[J].ISIJ International,2013,53(8):1411- 1419.
[13]Nakai Y,Sumil,Kikuchi N,et al.Powder Blasting in Hot Metal Desulfurization by Mechanical Stirring Process [J].ISIJ International,2017,57(6):1029- 1036.
[14] Takahashi K,Utagawa K,Shibata H,et al.Influence of Solid CaO and Liquid Slag on Hot Metal Desulfurization[J].Transactions of the lron& Steel Institute of Japan,2012,52(1):10- 17.
[15]喻同信,马星火,何 腾,等.降低KR脱硫剂单耗试验[J].中国冶金,2017,27(9):35-37.
[16]孙 亮,朱 良,赵晓东.3种铁水脱硫工艺的应用实践[J].中国冶金,2018,28(3):50-53.
[17]吴 明,李应江,单喷、复喷、KR法脱硫工艺在马钢的实践分析[J].中国冶金,2008,18(12);5.
|