塑料模具用1.2311预硬化特厚钢板的研制

韩飞1,2, 梁健3, 鲍思前1, 周练4   

  1. 1 武汉科技大学材料学部,武汉 430081;
    2 湖南华菱湘潭钢铁有限公司,湘潭 411101;
    3 广东雄峰模具钢材料科技有限公司,佛山 528311;
    4 湖南科技大学建筑与艺术设计学院,湘潭 411201;
  • 收稿日期:2024-07-25 出版日期:2025-03-30 发布日期:2025-03-13
  • 作者简介:韩飞(1985—),男,本科,工程师;

Development of Pre-hardened and Ultra-thick 1.2311 Steel Plate Used for Plastic Mold Steel

Han Fei1,2, Liang Jian3, Bao Siqian1, Zhou Lian4   

  1. 1 Faculty of Materials Science,Wuhan University of Science and Technology, Wuhan 430081,China;
    2 Hunan Valin Xiangtan Iron and Steel Co.,Ltd., Xiangtan 411101,China;
    3 Guangdong Xiongfeng Mold Steel Material Technology Co.,Ltd., Foshan 528311,China;
    4 School of Architecture and Art Design,Hunan University of Science and Technology, Xiangtan 411201, China;
  • Received:2024-07-25 Published:2025-03-30 Online:2025-03-13

摘要: 基于国内外市场需求,介绍了塑料模具用1.2311预硬化特厚钢板的研制过程。对1.2311钢进行了连续相变行为试验研究,并绘制出静态连续冷却转变曲线。经KR预处理→120 t转炉(留渣法冶炼控制碳含量0.20%~0.30%)→LF(精炼吹氩时间保持≥60 min)→VD(真空度不高于67 Pa,真空保持时间≥20 min)→450 mm板坯连铸(过热度8~15 ℃、拉速0.45 m/min)→板坯加热→5 000 mm轧机轧制(粗轧末3道次压下量之和≥140 mm)→-870~890 ℃正火→ACC控制冷却(水冷、空冷结合)→550~610 ℃回火,成功研制出≥150 mm规格塑料模具用1.2311预硬化特厚钢板。结果表明,全厚度布氏硬度偏差≤15HBW,硬度均匀性良好,钢板超声波探伤符合GB/T2970―2016中I级要求。各项综合性能指标满足研制要求。

关键词: 1.2311钢, 预硬化, 连续冷却转变曲线, 硬度

Abstract: Based on domestic and abroad market demands,this article introduces the development process of pre-hardened and ultra-thick 1.2311 steel plate used for plastic mold steel.Experimental study on continuous phase transformation behavior of 1.2311 steel was conducted,and a static continuous cooling transformation curve was drawn.By KR pretreatment→120 t converter (smelting using slag retention method can control carbon content within 0.20%-0.30%)→LF(refining argon blowing time ≥60 minutes)→VD (vacuum degree ≤67 Pa,vacuum holding time≥20 minutes)→450 mm slab continuous casting(low superheat of 8-15 ℃,low pulling speed of 0.45 m/min)→Slab heating→5 000 mm mill rolling (the sum of the last three pass reductions is ≥140 mm for rough mill)→870-890 ℃ normalizing process→ACC controlled cooling (combination of water cooling and air cooling)→550-610 ℃ tempering process,the pre-hardened and ultra-thick steel plate for plastic mold 1.2311 with a specification of ≥150 mm was successfully developed.The results show that a Brinell hardness deviation of ≤15HBW across the entire thickness,resulting in good uniformity of hardness,the ultrasonic testing of the plates meets the requirements of Level I in GB/T2970―2016.All comprehensive performance indicators meet the development requirements.

Key words: 1.2311 steel, Pre-hardened, CCT Curve, Hardness