ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2022, Vol. 43 ›› Issue (4): 75-81.

• 组织和性能 • 上一篇    下一篇

固溶和时效处理时间对IN706合金组织与性能的影响

张冰冰1,白亚冠1, 张鑫1,聂义宏2,3   

  1. 1天津重型装备工程研究有限公司,天津300457,
    2中国第一重型机械股份公司,齐齐哈尔161042;
    3黑龙江省高端核电装备智能制造重点实验室,齐齐哈尔161042
  • 收稿日期:2021-11-29 出版日期:2022-08-01 发布日期:2022-08-21
  • 作者简介:张冰冰(1994-),男,硕士(2020年北京科技大学),助理工程师,2017年河北科技大学(本科)毕业,大型镍基合金锻件开发。
  • 基金资助:
    黑龙江省自然科学基金杰出青年项目(JQ2021E007)

Effect of Solution and Aging Treatment Time on Structure and Mechanical Properties of IN706 Alloy

ZHANG Bingbing1, BAI Yaguan1, ZHANG Xin1, NIE Yihong2,3   

  1. 1 Tianjin Heavy Industries Research & Development Co Ltd, Tianjin 300457;
    2 China First Heavy Industries Co Ltd, Qiqiha'er 161042 ;
    3 Heilongjiang Provincial Key Laboratory of Intelligent Manufacturing for Advanced Nuclear Power Equipment, Qiqiha, er 161042
  • Received:2021-11-29 Published:2022-08-01 Online:2022-08-21

摘要: 研究了增加标准的980℃1h固溶-825℃ 2.5 h稳定化-720℃8 h+620℃8 h时效的处理时间对IN706合金(/%:0.03C,41Ni,16Cr,1.6Ti,2.9Nb)组织和性能的影响。结果表明,固溶处理时间(1~3 h)的增加,主要影响合金的晶粒尺寸,从而影响合金的性能;随稳定化处理时间(2.5~5 h)的增加,η相析出增多,导致强化相形成元素减少,合金性能亦有所下降,并对合金塑性和韧性产生不良影响;增加一级(8~18 h)和二级(8~36 h)时效处理的时间,会促进γ"和γ’相的析出,并且其形态也会发生变化,进而对合金的性能产生影响,但固溶1~3 h,稳定化2.5~5 h,以及一级时效8~18 h,二级时效8~36 h时合金的力学性能指标均满足标准要求。

Abstract: The influence of treated time of standard treated process 980 ℃ 1 h solid solution-825 ℃ 2. 5 h stabilizing- 720 ℃ 8 h +620 ℃ 8 h aging on the structure and properties of IN706 alloy (/% :0. 03C,41Ni,16Cr,l. 6Ti,2. 9Nb) is studied. The results show that with the increase of the solid solution treatment time (1 ~3 h) , the grain size of the alloy will be affected to a certain extent, thereby affecting the properties of the alloy; with the increase of the stabilizing treatment time (2. 5 ~5 h) , the precipitation of η increases, which leads to the reduction of strengthening phase forming elements, strength, plasticity and toughess of the alloy. Increasing the time of primary (8 ~18 h) and (8 ~36 h) secondary aging treatment will promote the precipitation of γ" and γ’ , and their morphology will also change, which will affect the properties of the alloy. But with solid solution for 1 ~3 h, stabilizing for 2. 5 ~5 h, primary aging for 8 ~18 h, secondary aging for 8 -36 h, the alloy mechanical properties all meet requirement of standard.

Key words:  , IN706 Alloy, Heat Treatment, Microstructure, Mechanical Properties