ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

特殊钢 ›› 2012, Vol. 33 ›› Issue (5): 12-14.

• 试验研究 • 上一篇    下一篇

RH精炼渣系和脱硫剂对管线钢脱硫影响的实验研究

姜桂连1,2,唐海燕1, 程爱民3, 李海顺3,王敬慧1,李京社1   

  1. 1北京科技大学冶金与生态工程学院,北京100083 ;
    2天津钢管集团有限公司炼钢厂,天津300301 ;
    3新兴铸管股份有限公司第一铸管部,武安056300
  • 收稿日期:2012-03-27 出版日期:2012-10-01 发布日期:2022-10-09
  • 作者简介:姜桂连(1959-),男,博士生,高级工程师,优质钢的质量控制研究。
  • 基金资助:
    教育部博士点(No. 20100006120008)和博士后基金 (20100480204)资助

Experimental Investigation on Effect of RH Refining Slag Series   and Desulfurization Agent on Desulfurization of Pipeline Steel

Jiang Guilian1,2, Tang Haiyan1 , Cheng Aiming3, Li Haishun3, Wang Jinhui1 , Li Jingshe1   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083;
    2 Steelmaking Plant, Tianjin Pipe Corp Ltd, Tianjin 300301;
    3 No! Ductile Pipe Dept, Xinxing Ductile Pipe Co Ltd, Wuan 056300
  • Received:2012-03-27 Published:2012-10-01 Online:2022-10-09

摘要: 以钢厂90 t RH精炼过程管线钢37Mn(/%:0.37C、0.21Si、1.44Mn、0.010P、0.003 4S)脱硫优化为目标,在实验室用GL-2型高温管式炉对原工厂用渣系:50CaO-35Al2O3-7SiO2-8MgO和脱硫剂:75.4CaO-20.1CaF2及优化渣系:57CaO-25Al2O3-10SiO2-8MgO和脱硫剂:70CaO-30CaF2共17个方案进行管线钢脱硫试验。结果表明,57CaO-25SAl2O3-10SiO2-8MgO精炼渣系和配合70CaO-30CaF2脱硫剂使用对钢液的脱硫效果最好,并且当渣量为5kg/t,脱硫剂量为0.7 kg/t时,能使钢液中的硫含量降到10×10-6

关键词: 管线钢37Mn, RH精炼, 精炼渣, 脱硫剂

Abstract: Aim to optimum-desulfurize the pipeline steel 37Mn (/%: 0. 37C, 0. 21 Si, 1. 44Mn, 0. 010P, 0.003 4 S) in 90t RH refining process at steelworks, in laboratory the desulfurization test on the pipeline steel with 17 schemes including original works slag series: 50CaO-35 Al2O33-7SiO2 -8 MgO and desulfurization agent: 75. 4CaO-20. 1CaF22and optimum slag series: 57CaO-25Al2O3-10SiO2-8MgO and desulfurization agent: 70CaO-30CaF2 has been carried out by a GL-2 type high temperature tubular resistance furnace. Results show that desulfurization effect of 57CaO-25Al2O3-10SiO2-8MgO refining slag series combined with 70CaO-30CaF2 desulfurization agent is best, and as slag amount is 5 kg/t steel combined with desulfurization agent of 0. 7 kg/t steel, the sulfur content in liquid could be decreased to 10 x 10-6.