ISSN:1003-8620

CN:42-1243/TF

主管:中信泰富特钢集团股份有限公司

主办:大冶特殊钢有限公司

组分对100 t LF高碱度精炼渣粘度和TC80钢脱硫的影响
赵青松, 仇圣桃, 赖朝彬, I张明博, 王晓晶
Effect of Ingredient on Viscosity of 100 t LF High Basicity Refining Slag and Desulphurization of steel TC80
Zhao Qingsong, Qiu Shengtao, Lai Chaobin , Zhang Mingbo, Wang Xiaojing
特殊钢 . 2016, (1): 43 -46 .