SCM435高强冷傲钢热轧过程中的再结晶行为
张永军, 韩静涛, 孔俊其, 侯月华, 郑永瑞, 李军, 甄琴英
Recrystallization Behavior of High Strength Cold Heading Steel SCM435 in Hot Rolling Process
Zhang Yongjun, Han Jingtao, Kong Junqi, Hou Yuehua, Zheng Yongrui, Li Jun, Zhen Qinying
特殊钢
.
2010, (1): 12
-13
.