重轨端部淬火温度场与相变的计算机模拟
张敏, 赵刚, 胡瑞海, 李文凯, 陈先舟, 楚双学, 董茂松
Computer Simulation on Temperature Field and Phase Transformation of Quenching Heavy Rail End
Zhang Min , Zhao Gang , Hu Ruihai , Li Wenkai , Chen Xianzhou , Chu Shuangxue, Dong Maosong
特殊钢
.
2010, (5): 14
-17
.