热处理工艺对核电站用SA-738Gr. B钢板组织和性能的影响
程含文, 赵国昌, 林明新, 谢东, 石莉, 肖雄峰
Effect of Heat Treatment Process on Structure and Properties of SA-738Gr. B Steel Plate for Nuclear Power Station
Cheng Hanwen, Zhao Guochang, Lin Mingxin, Xie dong, Shi Li , Xiao Xiongfeng
特殊钢
.
2021, (2): 56
-59
.