铁路轴箱轴承用8620钢3 t钢锭轧制产品研发
李博鹏, 陶士君, 张剑锋, 刘月云, 陆竹君, 吕文俊
Development of Rolled Steel Products from 3 t Ingot of Grade 8620 for Railway Axle Box Bearings
Li Bopeng , Tao Shijun, Zhang Jianfeng, Liu Yueyun, Lu Zhujun, Lv Wenjun
特殊钢
.
2024, (3): 1
-4
.
DOI: 10.20057/j.1003-8620.2023-00011