Zhang Yong,Sun Changliang,Liu Baoshi,et al.Effect of Electroslag Remelting Slag Systems on Non-metallic Inclusions in High-Quality Corrosion-Resistant Die Steel FS136[J].Special Steel,2026,47(05):42-47.
Zhang Yong,Sun Changliang,Liu Baoshi,et al.Effect of Electroslag Remelting Slag Systems on Non-metallic Inclusions in High-Quality Corrosion-Resistant Die Steel FS136[J].Special Steel,2026,47(05):42-47.DOI:10.20057/j.1003-8620.N260085.
Effect of Electroslag Remelting Slag Systems on Non-metallic Inclusions in High-Quality Corrosion-Resistant Die Steel FS136
Through the analysis of the chemical composition and non-metallic inclusions data of sampling experiments using two groups of different remelting slag systems to investigate the effect of electroslag remelting slag systems on non-metallic inclusion in corrosion-resistant die steel FS136, under identical experimental conditions, experiments with the binary(CaF
2
-Al
2
O
3
) and the quaternary(CaF
2
-Al
2
O
3
-CaO-MgO) slag systems showed no significant difference in alloying element loss. Metallographic observation and SEM analysis show that the non-metallic inclusions in FS136 steel are mainly Type D inclusions consist of Al
2
O
3
-based
granular inclusions. In FS136 steel processed with the quaternary experimental slag system, the Type D non-metallic inclusions were controlled to a rating level of 0.5–1.0. Compared with the binary slag system, the quaternary slag system exhibited better performance in wetting, absorption, and removal. The quaternary slag system can further improve the cleanliness of corrosion-resisant die steel FS136.
Brisenmark E . Formation and Evolution of Non-Metallic Inclusions in the Ladle Treatment-Ingot Casting-Electroslag Remelting Process Chain [D]. Stockholm, Sweden : KTH Royal Institute of Technology , 2024 .
Dong Y W , Jiang Z H , Yu A . Dissolution behavior of alumina-based inclusions in CaF 2 -Al 2 O 3 -CaO-MgO-SiO 2 slag used for the electroslag metallurgy process [J]. Metals , 2016 , 6 ( 11 ): 273 .
姜周华 . 高品质特殊钢电渣重熔技术 [M]. 北京 : 冶金工业出版社 , 2021 .
Walek J , Odehnalová A , Kocich R . Analysis of thermophysical properties of electro slag remelting and evaluation of metallographic cleanliness of steel [J]. Materials , 2024 , 17 ( 18 ): 4613 .
Comparative Study on Microstructure and Properties of V4-Series High-Speed Steel Manufactured by Electroslag Remelting, Powder Metallurgy and Spray Forming
Effect of Different Slag Systems on the Cleanliness of 1.2343 Hot‑Work Die Steel
Thermodynamic Analysis and Process Control of Aluminum and Titanium Burning Loss in R-26 Alloy during Electroslag Remelting (ESR)
Migration Law of Mg Element during Electroslag Remelting of Superalloys
Research Progress on Service Behavior and Performance Improvement Strategies of Hot-forging Die Steel
Related Author
Xu Huixia
Zeng Tao
Fang Xiaojie
Gu Jinbo
Di Yingnan
Jiang Haiqing
Tian Jialong
Yang Shouxing
Related Institution
State Key Laboratory of Advanced Special Steel
Special Steel Research Institute of Iron and Steel Research Institute Co., Ltd.
Tiangong International Co., Ltd., Danyang
Jiangsu Hongsheng Mold Steel Material Technology Co., Ltd.