Commercial Production Practice of Steel SA-210A1 for High Pressure Boiler by 100 t EAF-LF-VD Φ 500 mm Bloom Casting Flowsheet
特殊钢2018年39卷第3期 页码:25-27
作者机构:
山钢股份莱芜分公司特钢事业部,莱芜,271105
作者简介:
基金信息:
DOI:
中图分类号:
收稿:2017-11-30,
网络首发:2022-06-02,
纸质出版:2018-06-02
稿件说明:
移动端阅览
刘鹏. 100 t EAF-LF-VD Φ500 mm连铸坯流程高压锅炉用钢SA-210A1生产实践[J]. 特殊钢, 2018,39(3):25-27.
刘鹏. Commercial Production Practice of Steel SA-210A1 for High Pressure Boiler by 100 t EAF-LF-VD Φ 500 mm Bloom Casting Flowsheet[J]. Special Steel, 2018, 39(3): 25-27.
刘鹏. 100 t EAF-LF-VD Φ500 mm连铸坯流程高压锅炉用钢SA-210A1生产实践[J]. 特殊钢, 2018,39(3):25-27.DOI:
刘鹏. Commercial Production Practice of Steel SA-210A1 for High Pressure Boiler by 100 t EAF-LF-VD Φ 500 mm Bloom Casting Flowsheet[J]. Special Steel, 2018, 39(3): 25-27.DOI:
0.012~0.018Alt)的冶金工艺流程为55%铁水+废钢-100 t EAFLF-VDΦ500 mm坯连铸-轧制成Φ130mm圆钢。通过低铝脱氧工艺-EAF终点控制[C
]
≤0.06%
[P
]
0.006%~0.010%
出钢加石灰12 kg/t
AD粉(/%:10~13A1
55~60Al
2
O
3
5~8SiO
2
5~8Mg0)3 kg/t
700%Al钢芯铝3 kg/t预脱氧;LF采用5.76~6.06高碱度Al
2
O
3
渣系
LF终点喂0.40 kg/t钙线
软吹≥10 min;中间包钢水过热度15~25℃连铸结晶器和末端电磁搅拌
拉速0.31~0.32 m/min
铸坯缓冷≥48 h等工艺措施
SA-210A1钢中的[O
]
16×10
-6
~24×10
-6
[N
]
65×10
-6
~80×10
-6
[Alt
]
≤0.020%
铸坯和热轧圆钢低倍组织和非金属夹杂物均满足要求
Abstract
The metallurgical process flowsheet of produced steel SA-210A1 for high pressure boiler (/% : 0. 08 ~ 0. 11C
0.22 ~0.24Si
0. 72 ~0.74Mn
0. 007 ~0.010P
0.004 ~ 0.005S
0.010 〜0.015V
0.025 ~ 0.035Ti
0. 012 - 0. 018Alt) is 55% hot metal + scrap- 100 EAF-LF-VD-
Φ
500 mm bloom casting-hot rolling to Φ130 mm Round bar. With the process measures including low aluminium deoxidation process- EAF end controlling [C
]
≤ 0. 06% and [P
]
0. 006% ~0. 010%
adding lime 12 kg/t
AD powder (/% : 10 ~ 13A1
55 ~ 60Al
2
O
3
5 - 8SiO
2
5 ~8MgO) 3 kg/t and 70% Al aluminium cable steel 3 kg/t in tapping liquid for pre-oxidation ; using 5. 76 ~6. 06 high basicity Al
2
O
3
slag series in LF refining
feeding 0. 40 kg/t calcium wire at end of LF and sift stirring for ^10 min; super-heating extent of liquid in tundish 15 ~25 ℃,using mold and end electromagnetic stirring process in casting
casting speed 0. 31 ~0. 32 m/min and casting bloom slow cooling for "48 h
the steel SA-210A1 steel [O
]
is 16 x 10
-6
~24 x 10
-6
[N
]
is 65 x 10
-6
~ 80 x 10
-6
and [Alt
]
is ≤ 0. 020%
the macrostructure and nonmetallic inclusions in casting bloom and hot-rolled round bar all meet the requirements.