Effect of Nitrogen on Mechanical Properties of Retaining Ring Steel Mn18Cr18N at High Temperature
更新时间:2026-01-21
    • Effect of Nitrogen on Mechanical Properties of Retaining Ring Steel Mn18Cr18N at High Temperature

    • Special Steel   Vol. 26, Issue 6, Pages: 20-22(2005)
    • Received:15 June 2005,

      Online First:11 April 2023,

      Published:11 April 2005

    移动端阅览

  • 陈慧琴, 刘建生, 郭会光. Effect of Nitrogen on Mechanical Properties of Retaining Ring Steel Mn18Cr18N at High Temperature[J]. Special Steel, 2005, 26(6): 20-22. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Mechanical Properties of Thin Slab of Steel SPHC at High Temperature

Related Author

果晶晶
陈健
王书桓

Related Institution

邢台职业技术学院资源与环境工程系
中钢集团邢台机械轧辐有限公司
河北联合大学冶金与能源学院
0