Finite Element Simulation of Stress and Strain of Concasting Slab during Straightening
|更新时间:2026-01-21
|
Finite Element Simulation of Stress and Strain of Concasting Slab during Straightening
Special SteelVol. 27, Issue 6, Pages: 10-12(2006)
作者机构:
东北大学材料与冶金学院,沈阳,110004
作者简介:
基金信息:
DOI:
CLC:
Received:28 April 2006,
Online First:01 March 2023,
Published:01 March 2006
稿件说明:
移动端阅览
邢广厂, 朱苗勇, 林启勇, et al. Finite Element Simulation of Stress and Strain of Concasting Slab during Straightening[J]. Special Steel, 2006, 27(6): 10-12.
DOI:
邢广厂, 朱苗勇, 林启勇, et al. Finite Element Simulation of Stress and Strain of Concasting Slab during Straightening[J]. Special Steel, 2006, 27(6): 10-12.DOI:
Finite Element Simulation of Stress and Strain of Concasting Slab during Straightening
The finite element simulation of stress and strain of 230 mm slab with casting rate 1.0 m/min and 3 different roller ways layout-single-point
four-point and continuous straightening have been carried out by elastoplastic finite element method. The results showed that the equivalent Von Mises stress and horizontal stress of slab decreased in turn in single-point
four-point and continuous straightening; compared with single-point straightening
the each point straightening stress and strain rate decreases obviously in four-point straightening; and in continuous straightening
the equivalent plastic strain changes linearly in deformation area up to maximum value 1. 11% with lower equivalent plastic strain rate-about 5.5×10