Pilot Production with Dynamic Soft Reduction to Improve Composition Uniformity in Cast Bloom of Heavy Rail Steels
|更新时间:2026-01-21
|
Pilot Production with Dynamic Soft Reduction to Improve Composition Uniformity in Cast Bloom of Heavy Rail Steels
Special SteelVol. 30, Issue 3, Pages: 28-30(2009)
作者机构:
1. 包头钢铁集团公司技术中心,包头,014010
2. 北京科技大学.,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:27 November 2008,
Online First:24 November 2022,
Published:24 November 2009
稿件说明:
移动端阅览
李峰, 刘平, 白月琴, et al. Pilot Production with Dynamic Soft Reduction to Improve Composition Uniformity in Cast Bloom of Heavy Rail Steels[J]. Special Steel, 2009, 30(3): 28-30.
DOI:
李峰, 刘平, 白月琴, et al. Pilot Production with Dynamic Soft Reduction to Improve Composition Uniformity in Cast Bloom of Heavy Rail Steels[J]. Special Steel, 2009, 30(3): 28-30.DOI:
Pilot Production with Dynamic Soft Reduction to Improve Composition Uniformity in Cast Bloom of Heavy Rail Steels
A set of domestic dynamic soft reduction equipment was installed at No5 280 mm x 380 mm bloom concast- ing line at Baotou Steel
bv which the pilot production for heavy steels U71 Mn and U75 V has been carried out for more than one vear. Results showed that with suitable process conditions
the central carbon segregation in heavy rail steels improved obviously by using soft reduction technology: the index of central carbon segregation in cross section of bloom was ≤1.08
the fluctuation of index of carbon segregation along longitudinal central line of bloom appreciably decreased and the chenii- cal composition deviation of steel rail also decreased.