Calculating Model for Nitriding and Denitriding of Stainless Steel 304 in AOD Refining and Its Application
更新时间:2026-01-21
    • Calculating Model for Nitriding and Denitriding of Stainless Steel 304 in AOD Refining and Its Application

    • Special Steel   Vol. 30, Issue 5, Pages: 28-30(2009)
    • Received:15 April 2009,

      Online First:21 November 2022,

      Published:21 November 2009

    移动端阅览

  • 沈春飞, 蒋兴元, 尹世友, et al. Calculating Model for Nitriding and Denitriding of Stainless Steel 304 in AOD Refining and Its Application[J]. Special Steel, 2009, 30(5): 28-30. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Simulation of Material and Heat Balance of 150 t AOD Melting 430 Stainless Steel under Different Charge Conditions
Application and Numerical Simulation of Molten Steel Flow Field in Tundish for Alloy Steel Billet Concasting
Electroslag Remelting Technology of 10 t Ingot and Application of Secondary Current Swing Control
Development and Application of Lubrication Technology for Rolling Process
Analysis on Action and Reaction Force between Slab and Rollers at Segment of Dynamic Soft Reduction and Application in Casting

Related Author

Kang Congpeng
Chen Hongzhi
Xu Yongbin
Lu Xiaohui
王硕明
朱立光
刘志国
梁玫

Related Institution

Steelmaking Branch of WISDRI Engineering Research Incorporation Limited
Steelmaking Plant of Zenith Steel (Nantong) Group Company Limited
河北理工大学冶金能源学院
石家庄钢铁公司技术中心
邢台机械轧辊集团股份有限公司
0