A Study on Water Modeling of Ladle with Bottom Argon Blowing in Critical Slag Entrapment Condition
Special SteelVol. 30, Issue 2, Pages: 7-9(2009)
作者机构:
北京科技大学冶金与生态工程学院,北京,100083
作者简介:
基金信息:
DOI:
CLC:
Received:01 September 2008,
Online First:28 November 2022,
Published:28 November 2009
稿件说明:
移动端阅览
艾新港, 包燕平, 吴华杰, et al. A Study on Water Modeling of Ladle with Bottom Argon Blowing in Critical Slag Entrapment Condition[J]. Special Steel, 2009, 30(2): 7-9.
DOI:
艾新港, 包燕平, 吴华杰, et al. A Study on Water Modeling of Ladle with Bottom Argon Blowing in Critical Slag Entrapment Condition[J]. Special Steel, 2009, 30(2): 7-9.DOI:
A Study on Water Modeling of Ladle with Bottom Argon Blowing in Critical Slag Entrapment Condition
According to a 70 t ladle prototype at steel works
the water model with model-prototype linear scale ratio 1:2.75 has been established. The obtained critical blowing gas rate was 450 L/min by water modeling test to measure the rate of ladle bottom blowing argon in critical slag entrapment condition. The horizontal flow velocity of liquid surface in ladle with different gas blowing rate was measured in test to analyze the relation between horizontal flow velocity and liquid entrapped slag in ladle and get the liquid surface flow rate in critical slag entrapment condition being 0.652 m/s and its Weber index in that condition being 6.967. Using critical Weber index to calculate liquid surface flow velocity in critical slag entrapment condition and method to define the argon blowing rate for critical liquid entrapped slag by measuring the argon blowing rate up to liquid surface flow rate in critical slag entrapment condition are discussed in this paper.