Influence of Solution Treatment on Structure and Mechanical Properties of Duplex Stainless Steel 00Cr25Ni7Mo4N
|更新时间:2026-01-21
|
Influence of Solution Treatment on Structure and Mechanical Properties of Duplex Stainless Steel 00Cr25Ni7Mo4N
Special SteelVol. 30, Issue 3, Pages: 58-60(2009)
作者机构:
1. 北京科技大学冶金与生态工程学院,北京,100083
2. 宝山钢铁股份有限公司,上海,201900
作者简介:
基金信息:
DOI:
CLC:
Received:15 November 2008,
Online First:24 November 2022,
Published:24 November 2009
稿件说明:
移动端阅览
王晓峰, 陈伟庆, 毕洪运. Influence of Solution Treatment on Structure and Mechanical Properties of Duplex Stainless Steel 00Cr25Ni7Mo4N[J]. Special Steel, 2009, 30(3): 58-60.
DOI:
王晓峰, 陈伟庆, 毕洪运. Influence of Solution Treatment on Structure and Mechanical Properties of Duplex Stainless Steel 00Cr25Ni7Mo4N[J]. Special Steel, 2009, 30(3): 58-60.DOI:
Influence of Solution Treatment on Structure and Mechanical Properties of Duplex Stainless Steel 00Cr25Ni7Mo4N
Effect of phase proportion and solution temperature on structure and mechanical properties of steel 00Cr25Ni7Mo4N ( % : 0. 007 ~0.009C
24. 50 〜24. 84Cr
6.92 〜6.99Ni
3.65 〜3. 72Mo
0. 27 ~0. 30N) melted by vacuum induction furnace (6. 5 kg ingot) has been studied. Results showed that with increasing solution temperature from 1 050 °C to 1 200 °C
ferrite content in steel increased from 48% 〜50% to 53% 〜55% ; with increasing solution temperature from 1 050 °C to 1 100 °C
the strength of steel decreased while the elongation and impact toughness of steel increased
and with increasing the solution temperature from 1 100 °C to 1 200 °C
the strength of steel increased while the e- longation and impact toughness of steel decreased
so optimum temperature of the steel was 1 100 °C ±50°C.