A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace
Special SteelVol. 31, Issue 5, Pages: 8-10(2010)
作者机构:
1. 北京科技大学冶金与生态工程学院,北京,100083
2. 首钢技术研究院,北京,100043
作者简介:
基金信息:
DOI:
CLC:
Received:26 April 2010,
Online First:11 November 2022,
Published:11 November 2010
稿件说明:
移动端阅览
丁宁, 包燕平, 孙齐松, et al. A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace[J]. Special Steel, 2010, 31(5): 8-10.
DOI:
丁宁, 包燕平, 孙齐松, et al. A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace[J]. Special Steel, 2010, 31(5): 8-10.DOI:
A Test and Study on Water Modelling for Optimization of Bottom Argon Blowing Process of a 90 t Ladle Furnace
The effect of location and number of gas permeable brick and bottom argon supply rate on mixing time of liquid in a 90 t ladle furnace at steelworks has been tested and studied by using water model with 1:2.5 geometric resemble scale. Results show that the optimum ladle furnace gas permeable brick is located under dumping area of high level charging hopper
the slag material and alloy is directed adding at bare area to get higher melting rate and alloy yield; and the mixing time o£ liquid in ladle is shortest with bottom gas blowing rate 23. 89 L/min
it is available to deep desulphurization of liquid steel.
Numerical Simulation of Bottom Argon Blowing Process for 130 Ton Ladle
Effect of Different Argon Blowing Modes on Refining Effect of Molten Steel
Water Model Simulation Test for VOD Refining Process
Water Modelling Test of a Special Asymmetrical 12 strand 35 t Tundish and Optimization of Flow Control Device
Related Author
Li Qi
Qiu Guoxing
Wang Gongliang
Gao Peng
Li Rongxiang
Wang Xiaoying
Zhou Mingxing
Zheng Bing
Related Institution
School of Metallurgical Engineering, Xi'an University of Architecture and Technology
Hebei Iron and Steel Group Shigang Company
Whole Processes of High Quality Fastener Application Technology Research Center of Universities in Hebei Province, Hebei Taihang Iron and Steel Group Co.,Ltd.
Technology Innovation Center for High Quality Cold Heading Steel of Hebei Province, Hebei University of Engineering
College of Materials and Metallurgy, Liaoning Science and Technology University