Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel
|更新时间:2026-01-21
|
Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel
Special SteelVol. 31, Issue 2, Pages: 21-24(2010)
作者机构:
1. 河北理工大学冶金与能源学院,唐11J,063009
2. 唐山钢铁股份有限公司,唐山,063016
作者简介:
基金信息:
DOI:
CLC:
Received:19 October 2009,
Online First:16 November 2022,
Published:16 November 2010
稿件说明:
移动端阅览
曾亚南, 李俊国, 韩志杰, et al. Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel[J]. Special Steel, 2010, 31(2): 21-24.
DOI:
曾亚南, 李俊国, 韩志杰, et al. Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel[J]. Special Steel, 2010, 31(2): 21-24.DOI:
Experimental Study on Water Model for a 50 t Top and Bottom Combined Blown Converter at Tangsteel
top blowing rate and bottom blowing rate on bath mixing time
penetrating deptht impact area and splashing amount has been studied by orthogonal design test using 1: 6.35 water model for a 50 t top and bottom combined blown converter at Tang steel. Results show that as compared to original 4-hole oxygen lance
with using improved variable angle 4-hole oxygen lance the impact area in bath increases
the penetrating depth and splashing amount decrease while the mixing time decreases. For the 50 t top and bottom combined blown converter the real lance lever ≤1.3 m is available to decrease tap to tap time and increase intensity of bath stirring; and the mixing time and splashing amount decrease by controlling top blown rate 13 000 ~ 14 000 m