Thermodynamic Calculation and Experimental Research on Nitrogen Solubility in Austenite Stainless Steel
|更新时间:2026-01-21
|
Thermodynamic Calculation and Experimental Research on Nitrogen Solubility in Austenite Stainless Steel
Special SteelVol. 31, Issue 5, Pages: 1-4(2010)
作者机构:
1. 东北大学材料与冶金学院,沈阳,110004
2. 宝钢股份有限公司不锈钢事业部,上海,200431
作者简介:
基金信息:
DOI:
CLC:
Received:19 April 2010,
Online First:10 November 2022,
Published:10 November 2010
稿件说明:
移动端阅览
沈春飞, 蒋兴元, 李阳, et al. Thermodynamic Calculation and Experimental Research on Nitrogen Solubility in Austenite Stainless Steel[J]. Special Steel, 2010, 31(5): 1-4.
DOI:
沈春飞, 蒋兴元, 李阳, et al. Thermodynamic Calculation and Experimental Research on Nitrogen Solubility in Austenite Stainless Steel[J]. Special Steel, 2010, 31(5): 1-4.DOI:
Thermodynamic Calculation and Experimental Research on Nitrogen Solubility in Austenite Stainless Steel
The solubility of nitrogen in solid stainless steel 304
304L
301S and 301L (γ-phase) and in melts of austenite stainless steel has been calculated by using thermodynamic analysis method to get computational model for solubility of nitrogen in the steels
and the experimental research on nitriding behavior in four austenite stainless steels has been carried out by 1 kg MoSi electric resistance furnace with 33-100 kPa at 1520 ~1580 ℃. Results show that the solubility of nitrogen in y- phase in solid austenite stainless steels is highest; in cooling and solidifying process at normal pressure there is a transformation process from liquid phase
δ-phase to γ-phase; the nitrogen content in austenite steel shall decrease if supersaturated nitrogen to 8- phase in melt of stainless steel precipitates as gas bubble
so it is available to melt high nitrogen austenite stainless steel by using quick cooling at normal pressure or pressurized casting.