Effect of Non-Equilibrium Solidification on Length of Liquid-Solid Region at Solidifying Front of Concasting Bloom
|更新时间:2026-01-21
|
Effect of Non-Equilibrium Solidification on Length of Liquid-Solid Region at Solidifying Front of Concasting Bloom
Special SteelVol. 31, Issue 2, Pages: 25-28(2010)
作者机构:
1. 北京科技大学冶金与生态工程学院与循环冶金教育部重点实验室,北京1000083
2. 中冶连铸技术工程股份有限公司,北京,100081
作者简介:
基金信息:
DOI:
CLC:
Received:02 November 2009,
Online First:16 November 2022,
Published:16 November 2010
稿件说明:
移动端阅览
钱宏智, 兰鹏, 张家泉, et al. Effect of Non-Equilibrium Solidification on Length of Liquid-Solid Region at Solidifying Front of Concasting Bloom[J]. Special Steel, 2010, 31(2): 25-28.
DOI:
钱宏智, 兰鹏, 张家泉, et al. Effect of Non-Equilibrium Solidification on Length of Liquid-Solid Region at Solidifying Front of Concasting Bloom[J]. Special Steel, 2010, 31(2): 25-28.DOI:
Effect of Non-Equilibrium Solidification on Length of Liquid-Solid Region at Solidifying Front of Concasting Bloom
The model of finite differential method for solutes micro-segregation during solidification of steel has been established by analysis on representative regular hexagonal dendrite structure micro-segregation model combined with applied steel grades. Non-equilibrium solidus lines calculated by established model coincide with the related experimental data published by Jemkontoret. The application of heat transfer calculating model for 280 mm x380 mm casting bloom of 0. 20C steel
0. 45C steel and U71Mn steel show that the length of liquid-solid region at center of bloom calculated by non-equilibrium solidus is longer than that calculated by equilibrium solidus and it increases with increasing carbon content in steel ; and the revised solidification parameters and established model are more precise to reflect the solidification process.