Effect of Fluid Flow Control Devices on Optimization of Flow Field in Tundish for Slab Casting
更新时间:2026-01-21
    • Effect of Fluid Flow Control Devices on Optimization of Flow Field in Tundish for Slab Casting

    • Special Steel   Vol. 31, Issue 2, Pages: 17-20(2010)
    • Received:12 October 2009,

      Online First:16 November 2022,

      Published:16 November 2010

    移动端阅览

  • 冯捷, 唐德池, 包燕平, et al. Effect of Fluid Flow Control Devices on Optimization of Flow Field in Tundish for Slab Casting[J]. Special Steel, 2010, 31(2): 17-20. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Application and Numerical Simulation of Molten Steel Flow Field in Tundish for Alloy Steel Billet Concasting
Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish
Optimum of Mould Taper Design for Slab Casting of Austenite Stainless Steel
Production   Practice of  150 mm×150 mm  Concasting Billet of Steel  ML08Al
Numerical Simulation of Flow Field of Molten Steel in Tundish for Slab Concasting and Operation Optimization

Related Author

王硕明
朱立光
刘志国
梁玫
Wang Cun
Chen Yongfeng
Yang Shufeng
Liu Wei

Related Institution

东北大学材料与冶金学院
河北理工大学冶金能源学院
石家庄钢铁公司技术中心
Beijing Aobang Advanced Materials Co., Ltd., Beijing
Xinxing Ductile Iron Pipes Co., Ltd.
0