Industrial Test on Energy Integration by Trans-scale in 150 t Electric Arc Furnace Steelmaking
|更新时间:2026-01-21
|
Industrial Test on Energy Integration by Trans-scale in 150 t Electric Arc Furnace Steelmaking
Special SteelVol. 31, Issue 3, Pages: 41-43(2010)
作者机构:
1. 北京科技大学冶金与生态工程学院,北京,100083
2. 天津钢管集团股份有限公司,天津,300301
作者简介:
基金信息:
DOI:
CLC:
Received:11 December 2009,
Online First:07 November 2022,
Published:07 November 2010
稿件说明:
移动端阅览
郁健, 李士琦, 孙开明, et al. Industrial Test on Energy Integration by Trans-scale in 150 t Electric Arc Furnace Steelmaking[J]. Special Steel, 2010, 31(3): 41-43.
DOI:
郁健, 李士琦, 孙开明, et al. Industrial Test on Energy Integration by Trans-scale in 150 t Electric Arc Furnace Steelmaking[J]. Special Steel, 2010, 31(3): 41-43.DOI:
Industrial Test on Energy Integration by Trans-scale in 150 t Electric Arc Furnace Steelmaking
跨尺度集成的方法取得了较好的生产效果:平均出钢量141.2 t;冶炼电耗314.3 kWh/t;氧气消耗41.0 m
3
/t
氧气利用率87.7%;金属收得率88.5%;冶炼周期49.5 min。
Abstract
Based on space-time multi-scale structure during material transformation process in melting and its effects
the 150 t electric arc furnace steelmaking process at Tianjin Pipe Co has been studied to realize the trans-scale energy integration of two unit- electric power supplying and oxygen supplying at working-level and to get math model for trans-scale energy integration at working-level. The results of 20 heats commercial test with quaternary charge structure show that better production effect is got by using the trans-scale energy integration's method
i. e. average tapping liquid amount 141. 2 t; electric power consumption for melting 314. 3 kWh/t; oxygen consumption 41. 0 m
3
/t; oxygen efficiency 87. 7% ; metal yield 88. 5% and tap-to-tap time 49. 5 min.