Present Status of Research and Development of High Strength Non-Quenched and Tempered Cold Heading Steels
|更新时间:2026-01-21
|
Present Status of Research and Development of High Strength Non-Quenched and Tempered Cold Heading Steels
Special SteelVol. 31, Issue 5, Pages: 26-28(2010)
作者机构:
1. 北京科技大学材料科学与工程学院,北京,100083
2. 安徽工业大学材料科学与工程学院,马鞍山,243002
作者简介:
基金信息:
DOI:
CLC:
Received:09 March 2010,
Online First:11 November 2022,
Published:11 November 2010
稿件说明:
移动端阅览
曹杰, 刘雅政, 阎军, et al. Present Status of Research and Development of High Strength Non-Quenched and Tempered Cold Heading Steels[J]. Special Steel, 2010, 31(5): 26-28.
DOI:
曹杰, 刘雅政, 阎军, et al. Present Status of Research and Development of High Strength Non-Quenched and Tempered Cold Heading Steels[J]. Special Steel, 2010, 31(5): 26-28.DOI:
Present Status of Research and Development of High Strength Non-Quenched and Tempered Cold Heading Steels
According to the present status of research and development of high strength non-quenched and tempered cold heading steel at home and abroad
the chemical composition
characteristics of process
structure and mechanical properties of 800 ~ 1200 MPa high strength non-quenched and tempered cold heading steels are analyzed and discussed. The high strength non-quenched and tempered cold heading steel should has high strength and excellent cold-forming property
of which the strength and hardness of hot rolled products should be controlled in a suitable range. The steel grade can get better structure and mechanical properties by using low carbon high manganese and micro-alloying steel series with thermal-mechanical control rolling process.